Conducting UV wood coating and preparation method thereof
A woodware coating and manufacturing method technology, used in conductive coatings, fire-retardant coatings, antifouling/underwater coatings, etc., can solve the problems of uncomplimentary high temperature resistance, adverse environmental effects, inconvenient use, etc., and improve impact resistance. , Improve the film forming efficiency and improve the effect of film forming rate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026]A conductive UV wood coating, the conductive UV wood coating is divided into pre-sequence coating components and follow-up coating components, wherein the pre-sequence coating components are chitosan antibacterial gel 8Kg by weight; follow-up coating components are composed of In parts by weight, 75Kg of an aqueous solution containing 15% unsaturated polyether polyol by mass fraction, 10Kg of aqueous solution of polyester polyol containing 25% unsaturated group, and 0.5Kg of blocked isocyanate crosslinking agent , defoaming agent 0.1Kg, vinyltrimethoxyethoxysilane sealing agent 2Kg, the isopropyl myristate 6Kg that the mass fraction of dissolving is 10% graphene, from goat's horn 30Kg, separate by stewing and grind mechanically again The obtained mixture of keratin and sterol with a particle size of 10 μm-15 μm after powdering is obtained by saturation sealing with 2 Kg of vinyltrimethoxyethoxysilane sealing agent.
[0027] The manufacture method of above-mentioned UV co...
Embodiment 2
[0044] The whole is consistent with Example 1, the difference is:
[0045] A kind of conductive UV wood coating, this conductive UV wood coating is divided into pre-sequence coating component and follow-up coating component, wherein the preceding sequence coating component is chitosan antibacterial gel 5Kg by weight; Follow-up coating component is made of Containing mass fraction by weight is 80Kg of aqueous solution 80Kg of unsaturated group polyether polyol containing mass fraction, is the aqueous solution 12Kg of 30% unsaturated group polyester polyol, blocked isocyanate crosslinking agent 1Kg, 0.2Kg of defoaming agent, 3Kg of vinyltrimethoxyethoxysilane sealing agent, 8Kg of isopropyl myristate with a mass fraction of 10% graphene dissolved in it, separated by stewing and mechanically milled from 35Kg of goat horns The resulting mixture of keratin and sterol with a particle size of 10 μm-15 μm as the main body is obtained by saturation sealing with 3 Kg of vinyltrimethoxye...
PUM
Property | Measurement | Unit |
---|---|---|
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
ignition point | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com