Graphene composite material applied in preparing spinning rubber covered roller and preparation method thereof
A composite material and graphene technology, applied in the field of carbon materials, can solve problems such as impenetrability, and achieve the effects of reasonable component configuration, simple preparation method and stable chemical properties
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0019] Embodiment 1 is applied to prepare the graphene composite material of textile rubber roller
[0020] The graphene composite material applied to the preparation of textile cots comprises the following raw materials in parts by weight: 100 parts by weight of polyurethane, 32 parts by weight of graphene, 11 parts by weight of zinc acetate, 8 parts by weight of high-strength carbon fiber, 1 part by weight of antimony dioxide, 1 weight part of cobalt aluminate, 2 weight parts of electrolytic silver powder, 4 weight parts of styrene-acrylonitrile-styrene binary copolymer, 3 weight parts of epoxy fatty acid methyl ester, 3-7 weight parts of SDS mineral powder, 1 weight part of polyaluminum sulfate 2 parts by weight of cyclohexanone, 1 part by weight of 3-aminopropyltriethoxysilane, and 1 part by weight of ammonium methylsulfate (3-lauramidopropyl).
Embodiment 2
[0021] Embodiment 2 is applied to prepare the graphene composite material of textile rubber roller
[0022] The graphene composite material applied to the preparation of textile cots comprises the following raw materials in parts by weight: 100 parts by weight of polyurethane, 32 parts by weight of graphene, 11 parts by weight of zinc acetate, 8 parts by weight of high-strength carbon fiber, 1 part by weight of antimony dioxide, 1 part by weight of cobalt aluminate, 2 parts by weight of electrolytic silver powder, 4 parts by weight of styrene-acrylonitrile-styrene binary copolymer, 3 parts by weight of epoxy fatty acid methyl ester, 5 parts by weight of SDS mineral powder, 2 parts by weight of polyaluminum sulfate, 3 parts by weight of cyclohexanone, 3 parts by weight of 3-aminopropyltriethoxysilane, and 2 parts by weight of ammonium methylsulfate (3-lauramidopropyl)trimethyl.
Embodiment 3
[0023] Embodiment 3 is applied to prepare the graphene composite material of textile rubber roller
[0024] The graphene composite material applied to the preparation of textile cots comprises the following raw materials in parts by weight: 100 parts by weight of polyurethane, 32 parts by weight of graphene, 11 parts by weight of zinc acetate, 8 parts by weight of high-strength carbon fiber, 1 part by weight of antimony dioxide, 1 part by weight of cobalt aluminate, 2 parts by weight of electrolytic silver powder, 4 parts by weight of styrene-acrylonitrile-styrene binary copolymer, 3 parts by weight of epoxy fatty acid methyl ester, 7 parts by weight of SDS mineral powder, 3 parts by weight of polyaluminum sulfate, 4 parts by weight of cyclohexanone, 5 parts by weight of 3-aminopropyltriethoxysilane, and 3 parts by weight of ammonium methylsulfate (3-lauramidopropyl)trimethyl.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com