Modified asphalt concrete and its preparation method and construction method

A technology for modifying asphalt and concrete, which is applied in the field of concrete, and can solve problems not involved in the modification of asphalt concrete, and achieve the effect of ensuring correct elevation, avoiding pollution, and ensuring maintenance

Inactive Publication Date: 2020-02-21
BEIJING CHUANGTONG CONSTR GRP CO LTD
View PDF7 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] The Chinese patent with the application number CN201310513266.1 discloses a modified asphalt concrete with the function of cooling and reducing emissions, which is made of the following raw materials in parts by weight: 100 parts of ore, 4 to 8 parts of asphalt, 0.5 to 2.4 parts of iron ore powder parts, 0.01-0.05 parts of coupling agent; the iron ore powder is magnetite powder or / and maghemite powder, the coupling agent is a silane coupling agent, and the gradation type of the mineral material is AC -13 type, although this kind of modified asphalt concrete has the function of reducing emission and cooling, it can reduce the emission of pollutant gas during the mixing and paving process, and can reduce the temperature of the road surface in the summer high temperature season, but it does not involve low temperature resistance Modification of asphalt concrete

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0048] The raw materials of this embodiment include the following parts by weight: 350 parts of coarse aggregate, 70 parts of fine aggregate, 31 parts of asphalt, 38 parts of granulated blast furnace slag powder, 2 parts of super absorbent resin, 1.5 parts of wood fiber, 3.5 parts of glass fiber Parts, 2 parts of chitosan, 1 part of polyethylene oxide.

[0049] Step 1: Dry the coarse aggregate, fine aggregate, and filler after treatment, and preheat it to 170°C together, and heat the asphalt to 160°C for standby;

[0050] Step 2: First mix glass fiber and polyethylene oxide into the mixed aggregate after drying in step 1, and mix for 30 seconds, then add liquid asphalt and mix for 80 seconds, then add wood fiber and chitosan and mix for 100 seconds to obtain the result The loose mixture of modified asphalt concrete is described.

Embodiment 2

[0052] The raw materials of this embodiment include the following parts by weight: 365 parts of coarse aggregate, 73 parts of fine aggregate, 30 parts of asphalt, 40 parts of granulated blast furnace slag powder, 2.3 parts of super absorbent resin, 1.5 parts of wood fiber, 4 parts of glass fiber Parts, 3 parts of chitosan, 1.2 parts of polyethylene oxide.

[0053] The preparation method is:

[0054] Step 1: Dry the coarse aggregate, fine aggregate, and filler after treatment, and preheat it to 170°C together, and heat the asphalt to 160°C for use;

[0055] Step 2: First mix glass fiber and polyethylene oxide into the mixed aggregate after drying in step 1, and mix for 35 seconds, then add liquid asphalt and mix for 90 seconds, then add wood fiber and chitosan and mix for 110 seconds to obtain the result The loose mixture of modified asphalt concrete is described.

Embodiment 3

[0057] The raw materials of this embodiment include the following parts by weight: 370 parts of coarse aggregate, 80 parts of fine aggregate, 33 parts of asphalt, 42 parts of granulated blast furnace slag powder, 2.6 parts of super absorbent resin, 2.3 parts of wood fiber, 4.2 parts of glass fiber Parts, 3.5 parts of chitosan, 1.3 parts of polyethylene oxide.

[0058] Step 1: Dry the coarse aggregate, fine aggregate, and filler after treatment, and preheat it to 170°C together, and heat the asphalt to 160°C for standby;

[0059] Step 2: First mix glass fiber and polyethylene oxide into the mixed aggregate after drying in step 1, and mix for 25 seconds, then add liquid asphalt and mix for 90 seconds, then add wood fiber and chitosan and mix for 100 seconds to obtain the The loose mixture of modified asphalt concrete is described.

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
particle diameteraaaaaaaaaa
particle diameteraaaaaaaaaa
Login to View More

Abstract

The invention discloses a modified bituminous concrete and a preparation and construction method thereof. The modified bituminous concrete is composed of, by weight part, 350-400 parts of coarse aggregate, 70-100 parts of fine aggregate, 30-35 parts of asphalt, 40-50 parts of filler, 1-3 parts of wood fiber, 3-5 parts of glass fiber, 2-4 parts of chitosan and 0.5-2 parts of polyoxythylene. The preparation method of the modified bituminous concrete comprises, firstly, processing, drying and then preheating the coarse aggregate, the fine aggregate and the filler to 170 DEG C, and heating the asphalt to 160 DEG C; secondly, mixing and stirring the glass fiber into the mixture obtained in the first step for 25-35 seconds, then adding in liquid asphalt for stirring for 80-100 seconds, and then adding in the wood fiber and the chitosan for stirring for 100-120 seconds to obtain the modified bituminous concrete in a loose state; lastly, performing shaping through a roll-forming method. The modified bituminous concrete can maintain good temperature resistance at high or low temperature to effectively avoid asphalt volatilization at high temperature as well as concrete cracking at low temperature, prolong the service life of concrete and facilitate preparation.

Description

Technical field [0001] The invention relates to a concrete, more specifically, it relates to a modified asphalt concrete. Background technique [0002] With the rapid development of high-grade highway construction in my country, the development of asphalt pavement has become inevitable. This is mainly because asphalt pavement has many advantages compared with cement pavement: such as smooth surface, comfortable driving, low vibration, low noise, and construction period. Short, easy to maintain and repair, suitable for phased construction, etc. But the early damage is also very serious: problems such as potholes, oil flooding, pumping, rolling, packing, washboard, rutting, etc., especially the rutting problem of high temperature stability, especially in the southern region. [0003] The Chinese patent with application number CN201210317807.9 discloses a crack self-healing asphalt concrete, which includes coarse aggregate, fine aggregate, filler and asphalt, rigid fiber and flexible ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): C04B26/26C04B14/44C04B16/02C04B24/38C04B24/28C04B18/14C04B24/24
CPCC04B26/26C04B2111/0075C04B2111/343C04B14/02C04B18/167C04B14/28C04B18/141C04B24/24C04B16/02C04B14/44C04B24/38C04B24/281Y02W30/91
Inventor 秦永成来晓慧秦鹏林秦永余
Owner BEIJING CHUANGTONG CONSTR GRP CO LTD
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products