Embodiment 1
[0029] A kind of production technology of tencel fiber blanket, comprises the following steps:
[0030] 1) Yarn selection: Tencel fiber is used as plush yarn, and blended yarn of polyester draft yarn and milk protein fiber is used as ground yarn;
[0031] 2) Weaving: use a double-needle bed warp knitting machine to weave plush yarn and ground yarn to obtain a Tencel fiber blanket; The distance is 12-14mm. Use No. 1 and No. 6 bars to weave 4 needle weft inserts on the front and rear needle beds respectively, No. 2 and No. 5 bars to weave chain weaving on the front and rear needle beds respectively, and No. 3 and No. 4 bars are in the front The first and rear needle beds knit plush separately, and the knitting speed is 360r / min;
[0032] 3) Scouring: put the blanket in step 2) into the scouring solution for scouring; when scouring, the bath ratio is controlled at 1:50, the scouring temperature is 90°C, and the scouring time is 40 minutes. The formula of the scouring solution is...
Embodiment 2
[0038] A kind of production technology of tencel fiber blanket, comprises the following steps:
[0039] 1) Yarn selection: Tencel fiber is used as plush yarn, and blended yarn of polyester draft yarn and milk protein fiber is used as ground yarn;
[0040] 2) Weaving: use a double-needle bed warp knitting machine to weave plush yarn and ground yarn to obtain a Tencel fiber blanket; The distance is 12-14mm. Use No. 1 and No. 6 bars to weave 4 needle weft inserts on the front and rear needle beds respectively, No. 2 and No. 5 bars to weave chain weaving on the front and rear needle beds respectively, and No. 3 and No. 4 bars are in the front , the rear needle bed knit plush separately, the knitting speed is 400r / min;
[0041] 3) Scouring: put the blanket in step 2) into the scouring solution for scouring; control the bath ratio 1:50 during scouring, the scouring temperature is 95°C, and the scouring time is 50 minutes. The formula of the scouring solution is : Sodium silicate 0...
Embodiment 3
[0047] A kind of production technology of tencel fiber blanket, comprises the following steps:
[0048] 1) Yarn selection: Tencel fiber is used as plush yarn, and blended yarn of polyester draft yarn and milk protein fiber is used as ground yarn;
[0049] 2) Weaving: use a double-needle bed warp knitting machine to weave plush yarn and ground yarn to obtain a Tencel fiber blanket; The distance is 12-14mm. Use No. 1 and No. 6 bars to weave 4 needle weft inserts on the front and rear needle beds respectively, No. 2 and No. 5 bars to weave chain weaving on the front and rear needle beds respectively, and No. 3 and No. 4 bars are in the front , and rear needle beds respectively knit plush at a knitting speed of 440r / min;
[0050] 3) Scouring: put the blanket in step 2) into the scouring solution for scouring; when scouring, the bath ratio is controlled at 1:50, the scouring temperature is 100°C, and the scouring time is 60 minutes. The formula of the scouring solution is : Sodiu...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com