The preparation method of anion collector
An anionic collector and temperature control technology, applied in solid separation, flotation and other directions, can solve the problems of many impurities, reduced collection effect, waste of resources and environment, etc., achieve huge economic benefits, improve phosphorus collection rate, utilization The effect of discarding resources
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0023] This example relates to the anion collector of the present invention and its preparation.
[0024] The preparation method is as follows: Add the raw materials according to the established order, first stir the waste oil and heat up to 35-38°C, then add sodium petroleum sulfonate, continue to stir and heat up to 55-58°C, then add triethanolamine and phthalic acid di Methyl ester, keep stirring, control the temperature not to exceed 60°C, after all raw materials are fully fused into a uniform solution, add an aqueous solution with a temperature of 40±1°C and a pH value of 10, heat while stirring, control the temperature at 65°C-80 Carry out saponification reaction at ℃ for 20-30 minutes, wait until the material is translucent, then add surfactant fatty alcohol polyoxyethylene ether sodium sulfate (AES) or α-sulfo fatty acid methyl ester sodium salt (MES), and then After stirring for another 10 minutes until uniform, adjust the pH to 7.5±0.1 and lower to room temperature t...
Embodiment 2
[0029] This example relates to the performance evaluation of the anion collector of the present invention.
[0030] The anion collector of Example 1 is used to carry out flotation to the phosphorus-containing tailings obtained after iron flotation of phosphorite ore, and the flotation operation steps are as follows:
[0031] (1) Take the slurry from the phosphorite tailings after flotation in a mining site, divide it into several parts after wet mixing, and test its phosphorus grade;
[0032] (2) Using a 1.5L flotation machine in the laboratory, the roughing and sweeping impeller speeds are adjusted to 2000 rpm, and the selected impeller speeds are adjusted to 1500 rpm;
[0033] (3) According to figure 1 The shown test procedure and sequential dosing form a closed-circuit test procedure; the roughing and sweeping flotation time is 3 minutes, the refining 1 flotation time is 2 minutes, and the refining 2 and refining 3 flotation time are both 1.5 minutes;
[0034](4) The conc...
Embodiment 3
[0040] This embodiment relates to the performance comparison between the anion collector described in the present invention and the existing anion collector.
[0041] The anion collector of the present invention and the existing anion collector are used in the same flotation experiment, and the phosphorus-containing tailings obtained after iron flotation are carried out to flotation, and the flotation process is the same as Embodiment two, flotation result is:
[0042]
[0043] As can be seen from the results in the table above, the anion collector of the present invention is used for flotation of phosphorus-containing tailings obtained after iron flotation of ferrophosphorite, which can improve the phosphorus collection rate, improve the concentrate grade obtained, and make After the phosphorus tailings are floated by the anion collector of the present invention, the residual phosphorus grade is reduced to extremely low, and the phosphorus in the tailings can be eff...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com