Embodiment 1
[0031] An antibacterial modified back paint, consisting of the following components: polyester resin 16kg, solvent (the solvent is a mixed solvent of DBE and PMA, and the weight ratio of DBE to PMA is 1:1) 12kg, dispersant (SU263 macromolecule block Copolymer dispersant) 0.4kg, anti-settling agent (castor oil derivative) 0.4kg, rutile titanium dioxide 22kg, precipitated barium sulfate 5kg, 40wt% 609 epoxy solution 30kg, hemimethylated amino resin 12kg, 5265 urea-formaldehyde Resin 3kg, adhesion promoter (LTW) 3kg, acid catalyst (dinonyl naphthalene sulfonic acid) 0.8kg, orchid vanilla 25kg, flat wood 15kg, fragrant papaya 23kg.
[0032] The preparation method of described antibacterial modified back paint, the steps are:
[0033] 1) Take orchid vanilla, flat wood and fragrant papaya, crush them to 80 mesh, and extract them with analytically pure ethanol for 4 hours. After the extraction is completed, filter out the filter residue to obtain an antibacterial solution;
[0034] ...
Embodiment 2
[0039] An antibacterial modified back paint, consisting of the following components: polyester resin 10kg, solvent (the solvent is a mixed solvent of DBE and PMA, the weight ratio of DBE and PMA is 1:2) 6kg, dispersant (SU263 macromolecule block Copolymer dispersant) 0.1kg, anti-settling agent (organic bentonite) 0.1kg, rutile titanium dioxide 10kg, precipitated barium sulfate 2kg, 40wt% 609 epoxy liquid 15kg, hemimethylated amino resin 5kg, 5265 urea-formaldehyde resin 1kg , Adhesion promoter (LTW) 1kg, acid catalyst (p-toluenesulfonic acid) 0.1kg, orchid vanilla 20kg, flat wood 10kg, fragrant papaya 15kg.
[0040] The preparation method of described antibacterial modified back paint, the steps are:
[0041] 1) Take orchid vanilla, flat wood and fragrant papaya, grind them to 50 mesh, use analytically pure ethanol to extract for 3 hours, and filter out the filter residue to obtain the antibacterial liquid;
[0042] 2) Dissolving the polyester resin in a solvent to obtain a p...
Embodiment 3
[0045] An antibacterial modified back paint, consisting of the following components: polyester resin 30kg, solvent (the solvent is a mixed solvent of DBE and PMA, the weight ratio of DBE and PMA is 2:1) 20kg, dispersant (SU263 macromolecule block Copolymer dispersant) 1kg, anti-settling agent (organic bentonite) 1kg, rutile titanium dioxide 35kg, precipitated barium sulfate 10kg, 40wt% 609 epoxy liquid 40kg, hemimethylated amino resin 20kg, 5265 urea-formaldehyde resin 5kg, attached Accelerator (LTW) 5kg, acid catalyst (dodecylbenzene sulfonic acid) 1.5kg, orchid vanilla 30kg, flat wood 20kg, fragrant grass 30kg.
[0046] The preparation method of described antibacterial modified back paint, the steps are:
[0047] 1) Take orchid vanilla, flat wood and fragrant papaya, grind them to 100 mesh, use analytically pure ethanol to extract for 5 hours, after the extraction is completed, filter off the filter residue to obtain an antibacterial solution;
[0048] 2) Dissolving the pol...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com