Chelating adsorbent for blood purification and preparation method thereof
An adsorbent and chelating technology, which is applied in the field of chelating adsorbent for blood purification and its preparation, can solve the problems of reduced process production efficiency, poor blood compatibility, limitations, etc., and achieve improved adsorption and removal capacity with a simple method , the effect of structural simplification
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0032] A preparation method of chelating adsorbent for blood purification, including the following steps:
[0033] 1) Immerse the polymer in an organic solvent solution containing vinyl monomers and maleic anhydride for irradiation treatment;
[0034] 2) Remove unreacted monomer, maleic anhydride and organic solvent to obtain adsorbent;
[0035] Among them, the vinyl-containing monomer is selected from styrene, vinyl acetate or vinyl pyrrolidone.
[0036] Preferably, in the above preparation method, the adsorbent prepared in step 2) is further subjected to chloromethylation and amination, and then coupled to an anticoagulant; or the adsorbent prepared in step 2) is further subjected to sulfonation modification Sex.
[0037] Preferably, in the above preparation method, the organic solvent is at least one of acetone and methyl ethyl ketone.
[0038] Preferably, in the above preparation method, the polymer is porous sheet-shaped polyethylene, polyurethane, polycarbonate, microspherical pol...
Embodiment 1
[0047] 1) Take 1g polyethylene sheet (pore size 140um, you can directly use the products on the market), add 2.0wt% vinyl acetate, 2.5wt% maleic anhydride in acetone solution 50mL, use 60 Coγ-ray irradiation dose of 50kGy;
[0048] 2) After soaking and rinsing with acetone and 5% sodium hydroxide, then rinse with injection water.
Embodiment 2
[0050] 1) Take 1g polyethylene sheet (pore size 130um, you can directly use the products on the market), add 2.5wt% styrene, 2.5wt% maleic anhydride in acetone solution 50mL, use 60 Coγ-ray irradiation dose of 30kGy;
[0051] 2) After soaking and rinsing with acetone and 5% sodium hydroxide, then rinse with injection water.
[0052] After testing, the moisture content of the modified board cleaned by injection water was 68%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com