[0013] A heat-resistant and aging-resistant sheath material, prepared from the following raw materials in parts by weight (kg): low-density polyethylene 50, EVA resin 13, nylon 69, magnesium hydroxide 14, sodium methylene bis-naphthalene sulfonate 0.6 , titanate coupling agent 1021.3, organosilicon 5, organic montmorillonite 3, vinyl acetate 2, lithium nitride 4, paraffin oil 4, roasted zeolite powder 4, pentaerythritol phosphate 3, deionized water amount;
[0014] The heat-resistant and aging-resistant sheath material is prepared by the following specific steps:
[0015] (1) Dried magnesium hydroxide and mixed colloid mill with sodium methylene bis-naphthalene sulfonate for 10 minutes, then diluted titanate coupling agent 102 with an appropriate amount of ethanol, and sprayed the treated magnesium hydroxide powder Stir in a low-speed kneader at room temperature for 20 minutes, mix evenly and raise the temperature to 70°C, slowly add organic silicon and organic montmorillonite...
PUM
Property | Measurement | Unit |
---|---|---|
breaking strength | aaaaa | aaaaa |
electrical resistivity | aaaaa | aaaaa |
elongation at break | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com