Electronic element cleaning agent and preparation method thereof
A technology of electronic components and cleaning agents, applied in the field of cleaning agents, can solve the problems of poor chip cleaning effect and poor sewage treatment effect, etc.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] According to weight percentage, weigh 20% polyoxyethylene fatty alcohol, 3% diethanolamine, 3% organic phosphoric acid, 3% tripropylene glycol methyl ether, 1% antirust agent, 1% penetrating agent, .5% pH regulator, The remaining ingredients are deionized water.
[0024] Prepare each component according to the weight ratio, put polyoxyethylene fatty alcohol, diethanolamine, organic phosphoric acid, tripropylene glycol methyl ether, and deionized water into the mixer in order to mix, heat to 40 degrees, stir evenly, and then add anti Rust agent, penetrant, and pH regulator are stirred for 10-15 minutes.
Embodiment 2
[0026] According to the percentage by weight, weigh 23% polyoxyethylene fatty alcohol, 5% diethanolamine, 4% organic phosphoric acid, 4% tripropylene glycol methyl ether, 2% antirust agent, 2% penetrating agent, 0.8% PH regulator, and the rest The ingredients are deionized water.
[0027] Prepare each component according to the weight ratio, put polyoxyethylene fatty alcohol, diethanolamine, organic phosphoric acid, tripropylene glycol methyl ether, and deionized water into the mixer in order to mix, heat to 40 degrees, stir evenly, and then add anti Rust agent, penetrant, and pH regulator are stirred for 10-15 minutes.
Embodiment 3
[0029] According to the percentage by weight, weigh 20% polyoxyethylene fatty alcohol, 7% diethanolamine, organic 5% phosphoric acid, 5% tripropylene glycol methyl ether, 3% rust inhibitor, 2% penetrating agent, 1% pH regulator, and the rest The ingredients are deionized water.
[0030] Prepare each component according to the weight ratio, put polyoxyethylene fatty alcohol, diethanolamine, organic phosphoric acid, tripropylene glycol methyl ether, and deionized water into the mixer in order to mix, heat to 40 degrees, stir evenly, and then add anti Rust agent, penetrant, and pH regulator are stirred for 10-15 minutes.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com