Water type colorful coating

A multi-color paint, water-type technology, applied in the field of paint, can solve the problems of poor dispersibility, scrub resistance, friction resistance, etc., and achieve the effect of good dispersibility, good decorative effect and bright colors

Inactive Publication Date: 2014-10-01
苏州市超邦涂料有限公司
View PDF4 Cites 5 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0006] Aiming at the above technical problems, the present application provides a water-based colorful paint, which solves the technical ...

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0015] A kind of water-type colorful paint, its raw material ratio is as follows in parts by weight: 100 parts of hydroxyethyl cellulose; 15 parts of isopropanol; 20 parts of sodium hydroxide; 40 parts of xylene; 10 parts of sodium carboxymethyl cellulose ; 5 parts of lead naphthenate; 80 parts of deionized water; 15 parts of cobalt naphthenate; 10 parts of iron oxide green; 25 parts of modified bentonite; 20 parts of sodium polystyrene sulfonate; 10 parts of talcum powder; 4 parts of dibutyl formate; 30 parts of titanium dioxide; 10 parts of sodium naphthalenesulfonate; 20 parts of zinc phosphate.

[0016] Add hydroxyethyl cellulose, sodium hydroxide, xylene, sodium carboxymethyl cellulose and lead naphthenate to deionized water, heat to 40°C and stir for 3 hours, add cobalt naphthenate, modified bentonite, polystyrene Sodium sulfonate, talcum powder, sodium naphthalene sulfonate and dibutyl phthalate, heated up to 50°C and milled with a ball mill for 10 minutes, added isopro...

Embodiment 2

[0019] A kind of water-type colorful paint, its raw material ratio is as follows in parts by weight: 100 parts of hydroxyethyl cellulose; 25 parts of isopropanol; 30 parts of sodium hydroxide; 50 parts of xylene; 20 parts of sodium carboxymethyl cellulose ; 15 parts of lead naphthenate; 90 parts of deionized water; 35 parts of cobalt naphthenate; 20 parts of iron oxide red; 35 parts of modified bentonite; 40 parts of sodium polystyrene sulfonate; 30 parts of talcum powder; 10 parts of dibutyl formate; 40 parts of titanium dioxide; 20 parts of sodium naphthalenesulfonate; 30 parts of zinc phosphate.

[0020] Add hydroxyethyl cellulose, sodium hydroxide, xylene, sodium carboxymethyl cellulose and lead naphthenate to deionized water, heat to 40°C and stir for 3 hours, add cobalt naphthenate, modified bentonite, polystyrene Sodium sulfonate, talcum powder, sodium naphthalene sulfonate and dibutyl phthalate, heated up to 50°C and milled with a ball mill for 10 minutes, added isopro...

Embodiment 3

[0023] A kind of water-type colorful paint, its raw material ratio is as follows in parts by weight: 100 parts of hydroxyethyl cellulose; 20 parts of isopropanol; 25 parts of sodium hydroxide; 45 parts of xylene; 15 parts of sodium carboxymethyl cellulose ; 10 parts of lead naphthenate; 85 parts of deionized water; 25 parts of cobalt naphthenate; 15 parts of iron oxide yellow; 30 parts of modified bentonite; 30 parts of sodium polystyrene sulfonate; 20 parts of talcum powder; 7 parts of dibutyl formate; 35 parts of titanium dioxide; 15 parts of sodium naphthalenesulfonate; 25 parts of zinc phosphate.

[0024] Add hydroxyethyl cellulose, sodium hydroxide, xylene, sodium carboxymethyl cellulose and lead naphthenate to deionized water, heat to 40°C and stir for 3 hours, add cobalt naphthenate, modified bentonite, polystyrene Sodium sulfonate, talcum powder, sodium naphthalene sulfonate and dibutyl phthalate, heated up to 50°C and milled with a ball mill for 10 minutes, added isop...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses a water type colorful coating which is prepared from the following raw materials in parts by weight: 100 parts of hydroxyethyl cellulose, 15-25 parts of isopropanol, 20-30 parts of sodium hydroxide, 40-50 parts of xylene, 10-20 parts of sodium carboxymethylcellulose, 5-15 parts of lead naphthenate, 80-90 parts of deionized water, 15-35 parts of cobalt naphthenate, 10-20 parts of pigment, 25-35 parts of modified bentonite, 20-40 parts of sodium polystyrenesulfonate, 10-30 parts of talcum powder, 4-10 parts of plasticizer, 30-40 parts of titanium dioxide, 10-20 parts of naphthalene sulfonic acid and 20-30 parts of zinc phosphate. The product is bright and smooth in color, a coating film is resistant to scrubbing of 12000-13000 times without exposing a substrate, the dispersibility is good, no bobbles are caused and no powder drops off when the product is soaked in water of 20 DEG C for 40-60 days, the consumption of a reciprocating testing machine of 1000 times is 0.004-0.006g/cm<2>, the coating film is bright in color and good in decoration effect after being stored for 6-10 months at 25 DEG C, and thus the coating can be widely produced to constantly replace a conventional material.

Description

technical field [0001] The application belongs to the field of coatings, in particular to a water-based colorful coating. Background technique [0002] Paint, traditionally called paint in China. The so-called paint is coated on the surface of the object to be protected or decorated, and can form a continuous film firmly attached to the object to be coated, usually based on resin, oil, or emulsion, with or without adding pigments, fillers, adding Corresponding additives, viscous liquid prepared with organic solvent or sodium carboxymethyl cellulose. The relatively authoritative book "Painting Technology" in the Chinese coatings industry defines it as follows: "Painting is a material that can be coated on the surface of an object by different construction techniques to form a firm adhesion, a certain strength, and a continuous coating. Solid film. The film formed in this way is commonly called a coating film, also known as a paint film or a coating." The material coated on ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): C09D101/28C09D5/29C09D7/12
Inventor 费金华
Owner 苏州市超邦涂料有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products