A technology of brassinolide and suspension seed coating agent, applied in botany equipment and methods, seed coating/seed dressing, biocide, etc., can solve the problems of low dosage, low utilization rate, flying dust, etc. , to achieve the effects of promoting growth adjustment, high utilization rate of pesticides, and low environmental pollution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0045] Example 1: 0.3% Matrine-Brassinolide Suspension Seed Coating
[0046] 0.29 g of matrine, 0.01 g of brassinolide, 5 g of alkylphenol polyoxyethylene ether, 4 g of ethylene glycol, 0.15 g of xanthan gum, 1.0 g of white carbon black, 0.5 g of defoamer, and 0.1 g of mold agent, 3.0 g of everlasting red, 3 g of film-forming agent, 10 g of kaolin, 0.1 g of sorbic acid, and make up to 100 g of water. After stirring and mixing all the materials, grind them in a sand mill for 2 hours (rotating speed 2000-5000 / min) to obtain a magenta flowable suspension liquid, which is the finished product.
Embodiment 2
[0047] Example 2: 2.51% Matrine-Brassinolide Suspension Seed Coating
[0048] 25 kg of matrine, 0.1 kg of brassinolide, 20 kg of alkylnaphthalene sulfonate formaldehyde condensate sodium salt; 30 kg of alkylphenol polyoxyethylene ether, 40 kg of glycerin, and 10 kg of magnesium aluminum silicate , 5 kg of defoaming agent, 5 kg of antifungal agent, 10 kg of bentonite, 0.2 kg of citric acid, 2 kg of acid orange, and 850 kg of water.
[0049] All raw materials are put into a 1000L high-shear emulsification and dispersion kettle, fully emulsified and dispersed under airtight conditions, so that the slurry is more uniform and refined. Then transport the slurry to a sand mill for grinding, and the grinding material enters a blending kettle, then add 150 kg of 10% polyvinyl alcohol aqueous solution, stir and mix for 30 minutes, and then discharge. The obtained orange-yellow flowable suspension liquid is weighed and packaged to obtain the finished product.
Embodiment 3
[0050] Example 3: 10.03% matrine-brassinolide suspension seed coating
[0051] Matrine 10%
[0052] Brassinolide 0.03%
[0053] Sodium lignosulfonate 3%
[0054] Alkyl naphthalene sulfonic acid formaldehyde condensate sodium salt 5%
[0055] Styrylphenyl ethoxylate 2%
[0056] Glycerol 5%
[0057] Magnesium Aluminum Silicate 1.0%
[0058] Seed coating film former (853) 3%
[0059] 2% Xanthan Gum 5%
[0060] Bentonite 3%
[0061] Sorbic acid 0.2%
[0062] Acid Red B 2%
[0063] Defoamer 0.5%
[0064] Mold inhibitor 10%
[0065] Water to make up to 100%
[0066] According to the formula requirements, with water as the medium, 300 kg of matrine, 0.9 kg of brassinolide, 90 kg of sodium lignosulfonate, 150 kg of alkyl naphthalene sulfonate formaldehyde Condensate sodium salt, 60 kg styrylphenyl polyoxyethylene ether, 150 kg glycerin, 30 kg magnesium aluminum silicate, 90 kg seed coating agent film-forming agent (853), 90 kg bentonite, 6 kg sorbic acid , 60 kg of aci...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com