A film coating agent and tablet technology, which is applied in the field of pharmaceutical excipients, can solve problems such as the unsatisfactory moisture-proof effect of traditional Chinese medicine tablets and the inability to completely solve the problem of moisture absorption of traditional Chinese medicine, so as to solve the problem of moisture absorption, enhance moisture-proof performance, and expand the scope of use Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0016] A preparation method of a moisture-proof film coating agent for traditional Chinese medicine tablets, comprising the following steps:
[0017] (1) Throw vinylpyrrolidone-vinyl acetate copolymer, 5-15 centipoise hypromellose, polyethylene glycol 6000, iron oxide, titanium dioxide and talc into a high-speed mixer at a speed of 2700 rpm Mix for 0.5 to 3 minutes; the speed of the high-speed mixer is 2700 rpm, and the mixing time is 0.5 to 3 minutes.
[0018] (2) Sprinkle Tween 80 evenly on the material in the high-speed mixer, and mix at a speed of 2700 rpm for 0.5-3 minutes to make a finished Chinese medicine tablet moisture-proof film coating agent.
Embodiment 1
[0020] A preparation method of a moisture-proof film coating agent for traditional Chinese medicine tablets, comprising:
[0021] (1) Weigh 20 parts of vinylpyrrolidone-vinyl acetate copolymer, 30 parts of hypromellose of 5-15 centipoise, 600020 parts of polyethylene glycol, 803 parts of Tween, iron oxide 10 parts, 17 parts of talcum powder;
[0022] (2) Put vinylpyrrolidone-vinyl acetate copolymer, 5-15 centipoise hypromellose, polyethylene glycol 6000, iron oxide, titanium dioxide and talcum powder into a high-speed mixer, at a speed of 2700 Mix for 2 minutes at rpm;
[0023] (3) Sprinkle Tween 80 evenly on the material in the high-speed mixer, and mix at a speed of 2700 rpm for 15 minutes to prepare a moisture-proof film coating agent for traditional Chinese medicine tablets.
Embodiment 2
[0025] (1) Weigh 50 parts of vinylpyrrolidone-vinyl acetate copolymer, 10 parts of hypromellose of 5-15 centipoise, 600010 parts of polyethylene glycol, 803 parts of Tween, and 10 parts of iron oxide according to the ratio of parts by mass. 17 parts and talcum powder;
[0026] (2) Put 5-15 centipoise of hypromellose, polyethylene glycol 6000, iron oxide, titanium dioxide and talc into a high-speed mixer, and mix for 2 minutes at a speed of 2700 rpm;
[0027] (3) Sprinkle Tween 80 evenly on the material in the high-speed mixer, and mix at a speed of 2700 rpm for 15 minutes to prepare a film coating agent for Chinese medicine tablets.
[0028] Using a conventional method, a kind of moisture-proof film-coating agent for Chinese medicine tablets of Example 1 and Example 2 is made into a solution, and sprayed on the surface of the Chinese medicine core to make a moisture-proof film-coated tablet. Then carry out the moisture-proof test: use the constant temperature and humidity box...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com