Embodiment approach 1
[0188] Embodiment 1: Preparation of air-conditioning agent with iron powder and ferrous sulfate as main ingredients
[0189] Prepare iron powder, ferrous sulfate, sodium bicarbonate, bentonite, activated carbon (all above 100 mesh).
[0190] ①Water absorption by water-absorbing agent: Weigh NaCl, water and bentonite; mix and dissolve NaCl and water (reserve 1 / 5 of the water for iron powder activation), spray the obtained salt water into the bentonite, and stir evenly while spraying.
[0191] ②Make iron powder activator: weigh NH 4 Cl; NH 4 Dissolve Cl with reserved 1 / 5 water; weigh activated carbon, take half; add NH 4 The aqueous Cl solution was sprayed into the activated carbon taken out, and stirred evenly.
[0192] ③ Weigh sodium bicarbonate, ferrous sulfate, and iron powder; add sodium bicarbonate, ferrous sulfate, activated carbon (the other half), iron powder activator, and iron powder to the water-absorbing agent in sequence, and mix evenly. It is packaged with air...
Embodiment approach 2
[0193] Embodiment 2: Preparation of calcium chloride modified sepiolite and hemihydrate gypsum composite humidity control agent
[0194] Prepare sepiolite powder and hemihydrate gypsum powder (both above 100 mesh).
[0195] Dry the sepiolite powder at 100°C; weigh CaCl 2 , add an appropriate amount of water to fully dissolve, then mix with the dried sepiolite powder according to the ratio and stir evenly; after it becomes dry and loose, dry it at 110°C.
[0196] Mix calcium chloride-modified sepiolite powder with hemihydrate gypsum powder and water according to the formula; pour it into the mold, take it out from the mold after being formed, bake at 50°C for 5 hours; seal and package.
Embodiment approach 3
[0197] Embodiment 3: Preparation of calcium chloride modified attapulgite and white cement composite humidity control agent
[0198] Weigh CaCl 2 , add an appropriate amount of water to fully dissolve, then add attapulgite powder (above 100 mesh) according to the proportion, mix evenly, and bake at 105°C for 2 hours.
[0199] Mix the attapulgite powder modified by calcium chloride with white cement and water according to the formula; pour it into the mold, take it out from the mold after being formed, and bake it at 50°C for 4 hours; seal it and package it.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com