Method for preparing aromatic azoic compound by catalyzing aromatic amine with metal nanocrystals
A technology of metal nanocrystals and azo compounds, applied in chemical recycling, organic chemistry, etc., can solve the problems of non-recycling, poor catalyst universality, and low yield of aromatic azo compounds.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0036] The preparation method of the Ag nanocrystal that the present invention also provides, it follows the steps:
[0037] 1) In the state of stirring, add silver nitrate salt to octadecylamine at 80°C~100°C to make a solution with a mass ratio of 0.01~0.03g / g;
[0038] 2) In the state of stirring, add the above solution to octadecylamine at 180 ° C ~ 250 ° C for dilution to prepare a solution with a mass ratio of silver nitrate salt to octadecyl amine of 0.003 ~ 0.006 g / g;
[0039] 3) React for 10 to 60 minutes, cool down to 50°C to 80°C, add ethanol and precipitate precipitates, centrifuge and wash with ethanol to obtain Ag nanocrystals, and then disperse the obtained nanocrystals in cyclohexane for later use.
[0040] The present invention also provides the preparation method of described Au nanocrystal, it comprises the following steps:
[0041] 1) Dissolve chloroauric acid tetrahydrate in a mixed solvent of oleic acid and oleylamine at room temperature to make a soluti...
Embodiment 2
[0051] Implementation method: at room temperature, platinum acetylacetonate is added to oleylamine to prepare a solution with a volume concentration of 2 g / L. In the state of stirring, borane-tert-butylamine was added to the above solution to make a solution with a volume concentration of 6 g / L, and then the solution was transferred to a stainless steel autoclave with a polytetrafluoroethylene cup. Then the autoclave was kept at 150° C. for 2 hours and then cooled to room temperature. After adding ethanol, a precipitate was precipitated. After washing with ethanol, Pt nanocrystals were obtained, and then the obtained Pt nanocrystals were dispersed in cyclohexane for subsequent use.
Embodiment 3
[0053] Implementation method: at room temperature, add cobalt acetylacetonate salt into a mixed solvent of toluene and oleylamine to prepare a solution with a volume concentration of 1 g / L. In the state of stirring, borane-tert-butylamine was added to the above solution to make a 3 g / L solution, and then the solution was transferred to a stainless steel autoclave with a polytetrafluoroethylene cup. Then the autoclave was kept at 180 °C for 8 hours and then cooled to room temperature. After adding ethanol, a precipitate was precipitated. After washing with ethanol, Co nanocrystals were obtained, and then the obtained Co nanocrystals were dispersed in cyclohexane for later use.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com