Colored photoelastic polyester fine denier carpet yarn and preparation method thereof
A carpet yarn and photoelastic technology, which is applied in the field of carpet yarn, can solve the problems of reducing the linear density of monofilaments, and achieve the effects of improving cost performance, excellent color fastness, and strong covering power
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0031]BKV433POY high-speed spinning machine is used to spin colored and glossy fine-denier polyester filaments with single fiber linear density of 2.5dtex and multifilament linear density of 660dtex by using PET large glossy polyester chips and beige polyester masterbatch as raw materials. Multifilament, the spinning temperature is 295°C, and the spinning speed is 3500m / min; put the multifilament of the above-mentioned colored and bright fine denier polyester filament into the FK6M-700 type false twist setting machine for stretching, twisting and untwisting , After shaping, it is made into a highly fluffy three-dimensional crimped high-elastic deformed fiber, the deformation temperature is 200°C, the draft ratio: 1.8, the twist ratio (D / Y): 2.2, and the secondary setting temperature: 120°C; it will be deformed by false twisting The last two multifilament yarns with a linear density of 660dtex are combined into a single yarn with a linear density of 1320dtex by an Autoconer338 a...
Embodiment 2
[0034] BKV433POY high-speed spinning machine is used to spin the colored and glossy fine-denier polyester filament with single fiber linear density of 4dtex and multifilament linear density of 500dtex by spinning PET large glossy polyester chips and purple polyester masterbatch as raw materials. silk, the spinning temperature is 280°C, and the spinning speed is 3000m / min; the multifilament of the above-mentioned colored and bright fine-denier polyester filament is put into the FK6M-700 type false twist setting machine for stretching, twisting, untwisting, After shaping, it is made into a highly fluffy three-dimensional crimped high-elastic deformed fiber. The deformation temperature is 170°C, the draft ratio: 1.6, the twist ratio (D / Y): 2.0, and the secondary setting temperature: 160°C; Two multifilament yarns with a linear density of 500dtex are combined into a single yarn with a linear density of 1000dtex by an Autoconer338 automatic winder; the doubled single yarn is twisted...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com