Alcohol-soluble electromagnetic wave shielding coating
A technology of shielding coatings and electromagnetic waves, which is applied in the field of alcohol-soluble electromagnetic wave shielding coatings, can solve problems such as telephone noise, influence on the cardiovascular system, and information leakage, and achieve the effects of less harmful substances, a good working environment, and low VOC emissions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] The alcohol-soluble electromagnetic wave shielding paint of the present invention comprises the following components by weight percentage:
[0022]
[0023]
[0024] Use a disperser to disperse the alcohol-soluble acrylic conductive resin at high speed, add ethanol, and then mix the same prepared micron-sized silver-coated copper conductive powder, perform mechanical blending through high-speed dispersion, and then add γ-aminopropyl triethyl in turn Oxysilane, ammonium salt dispersant, antimony-tin oxide (ATO) nano-powder material, disperse at high speed for one hour, and mix evenly to obtain alcohol-soluble electromagnetic wave shielding coating.
Embodiment 2
[0026] The alcohol-soluble electromagnetic wave shielding paint of the present invention comprises the following components by weight percentage:
[0027]
[0028] Use a disperser to disperse the alcohol-soluble acrylic conductive resin at high speed, add ethanol, and then mix in the same prepared micron-sized pure silver conductive powder, perform mechanical blending through high-speed dispersion, and then add γ-aminopropyl triethoxy in turn Base silane, ammonium salt dispersant, antimony-tin oxide (ATO) nano-powder material, disperse at high speed for one hour, and mix evenly to obtain alcohol-soluble electromagnetic wave shielding coating.
Embodiment 3
[0030] The alcohol-soluble electromagnetic wave shielding paint of the present invention comprises the following components by weight percentage:
[0031]
[0032] Use a disperser to disperse the alcohol-soluble acrylic conductive resin at high speed, add ethanol, and then mix in the same prepared micron-sized nickel conductive powder, perform mechanical blending through high-speed dispersion, and then add γ-aminopropyl triethoxy in turn Silane, ammonium salt dispersant, antimony-tin oxide (ATO) nano-powder material, disperse at high speed for one hour, and mix evenly to obtain alcohol-soluble electromagnetic wave shielding coating.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
electrical resistivity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com