A hemostatic gel and suppository technology, applied in the directions of suppository delivery, blood diseases, cardiovascular system diseases, etc., can solve the problems of secondary bleeding, bleeding ineffective, etc., and achieve the effects of accelerating blood coagulation, being easy to accept, and inhibiting bacterial growth.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] In 1000g of hemostatic gel suppositories:
[0014] (1) Mix 380g sodium carboxymethylcellulose, 150g sodium alginate, and 400g polyvinyl alcohol;
[0015] (2) Add 50 g of glycerin, 20 g of Tween-80, and 2000 ml of deionized water into (1), and fully stir at a temperature of 50° C. to 90° C. to prepare a composite gel suppository raw material;
[0016] (3) When the temperature of the suppository raw material drops to 45°C, it is injected into a mold for molding, and after cooling and solidifying, a hollow thin-shell suppository is obtained.
Embodiment 2
[0018] In 1000g of hemostatic gel suppositories:
[0019] (1) 320g sodium carboxymethylcellulose, 300g chitosan, 300g polyvinyl alcohol are mixed;
[0020] (2) Add 60g of glycerin, 20g of Tween-80, and 2000ml of deionized water into (1), and fully stir at a temperature of 50°C to 90°C to prepare the composite gel suppository raw material;
[0021] (3) When the temperature of the suppository raw material drops to 45°C, it is injected into a mold for molding, and after cooling and solidifying, a hollow thin-shell suppository is obtained.
Embodiment 3
[0023] In 1000g of hemostatic gel suppositories:
[0024] (1) 400g sodium carboxymethylcellulose, 130g carbomer, 400g polyvinyl alcohol are mixed evenly;
[0025] (2) Add 50 g of glycerin, 20 g of Tween-80, and 2000 ml of deionized water into (1), and fully stir at a temperature of 50° C. to 90° C. to prepare a composite gel suppository raw material;
[0026] (3) When the temperature of the suppository raw material drops to 45°C, it is injected into a mold for molding, and after cooling and solidifying, a hollow thin-shell suppository is obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com