a laminated film, easy peeling technology, applied in the direction of film/foil adhesives, synthetic resin layered products, transportation and packaging, etc., can solve the problems of easy peeling, easy breakage of surface materials, inferior water resistance, etc., to achieve easy peeling and laminate
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Benefits of technology
Problems solved by technology
Method used
Examples
example 1
[0084] After each of thermoplastic resin composition d as layer (B), thermoplastic resin composition b as layer (A1), and thermoplastic resin composition c as layer (A2) was kneaded in each extruder set at 230.degree. C., they were supplied to a co-extrusion die set at 250.degree. C., laminated in the die and extruded in a sheet. The laminate was cooled by a cooler, thereby a three-layer unstretched sheet was obtained. The unstretched sheet was heated at 130.degree. C. and stretched 5 times in the machine direction.
[0085] The above sheet was cooled to a temperature of 60.degree. C., again heated to a temperature of 150.degree. C. and stretched 8.0 times in the transverse direction in a tenter oven, subjected to annealing treatment at a temperature of 162.degree. C., cooling at 60.degree. C., and corona discharge treatment, and then trimming, thereby a laminated film of a three-layer structure [(B) / (A1) / (A2): 1 / 49 / 10 .mu.m in thickness, stretched layer constitution: biaxial / biaxial / b...
example 2
[0086] After each of thermoplastic resin composition d as layer (B) and thermoplastic resin composition b as layer (A1) was kneaded in each extruder set at 230.degree. C., they were supplied to a co-extrusion die set at 250.degree. C., laminated in the die and extruded in a sheet. The laminate was cooled by a cooler, thereby a two-layer unstretched sheet was obtained. The unstretched sheet was heated at 130.degree. C. and stretched 4 times in the machine direction.
[0087] Thermoplastic resin composition b as layer (A2) was kneaded in an extruder set at 250.degree. C. and extruded in a sheet, and this sheet was laminated on the above-prepared 4 time-stretched film (A1), thereby a three-layer structure laminated film was obtained. The three-layer structure laminated film was cooled to a temperature of 60.degree. C., again heated to about 160.degree. C. by a tenter oven and stretched 7.5 times in the transverse direction, subjected to annealing treatment in a heat-set zone adjusted to 1...
example 3
[0088] After each of thermoplastic resin composition f as layer (B), thermoplastic resin composition b as layer (A1), and thermoplastic resin composition c as layer (A2) was kneaded in each extruder set at 240.degree. C., they were supplied to a co-extrusion die set at 270.degree. C., laminated in the die and extruded in a sheet. The laminate was cooled by a cooler, thereby a three-layer unstretched sheet was obtained. The unstretched sheet was heated at 120.degree. C. and stretched 5 times in the machine direction, subjected to annealing treatment at 160.degree. C., corona discharge treatment, and then trimming, thereby a laminated film of a three-layer structure [(B) / (A1) / (A2): 4 / 46 / 10 .mu.m in thickness, stretched layer constitution: monoaxial / monoaxial / monoaxial] having a thickness of 60 .mu.m, a peeling strength of 90 g / cm, and an opaqueness of 87% was obtained.
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com