[0053] Put magnesium tourmaline powder 100g, anatase nano-TiO 2 40g, rare earth oxide CeO 2 60g and 3.0 g of silver nitrate were prepared into a 60% slurry with deionized water. The prepared slurry was ground in a high-energy planetary ball mill at a speed of 350 rpm for 12 hours at a high speed. Dry the ground powder slurry at 100°C to remove the moisture in the slurry. Calcined at 600°C for 4 hours to make nano-TiO 2 , rare earth compounds and Ag ions are supported on tourmaline. Grinding on a high-energy planetary ball mill to a particle size of ≤5 μm, then grading and packaging to obtain the inorganic antibacterial agent.
example 2
[0055] Put magnesium tourmaline powder 100g, anatase nano-TiO 2 40g, rare earth complex CeO 2 +Ce(NO 3 ) 3 57g, 3.0g of silver nitrate, prepared into 60% slurry with deionized water. The prepared slurry was ground in a high-energy planetary ball mill at a speed of 350 rpm for 12 hours at a high speed. Dry the ground powder slurry at 150°C to remove the moisture in the slurry. Calcined at 600°C for 4 hours to make nano-TiO 2 , rare earth compounds and Ag ions are supported on tourmaline. Grinding on a high-energy planetary ball mill to a particle size of ≤5 μm, then grading and packaging to obtain the inorganic antibacterial agent.
example 3
[0057] Ferrite powder 140g, nano TiO 2 20g, rare earth oxide LaO 2 36g, 4.0g of zinc oxide, prepared into a 60% slurry with deionized water. The prepared slurry was ground in a high-energy planetary ball mill at a speed of 350 rpm for 24 hours at a high speed. Dry the ground powder slurry at 150°C to remove the moisture in the slurry. Calcined at 800°C for 4 hours to make nano-TiO 2 , rare earth compounds and zinc oxide loaded on tourmaline. Grinding on a high-energy planetary ball mill to a particle size of ≤5 μm, then grading and packaging to obtain the inorganic antibacterial agent.
PUM
Property | Measurement | Unit |
---|---|---|
diameter | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com