A technology of finishing agent and adhesive, which is applied in fiber treatment, biochemical fiber treatment, textiles and papermaking, etc. It can solve the problems of improper storage, bacteria breeding, residual glue, etc., and achieves wide application, strong production adaptability and dust removal. high efficiency effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0046] A sticky finishing agent, the composition of which is as follows: the adhesive includes 45kg of acrylic latex (glass transition temperature of -45°C), 5kg of polyvinyl alcohol (glass transition temperature of 80°C), calculated by the FOX formula, and bonded after mixing The glass transition temperature of the agent is about -36.6°C, 0.2kg of quaternary ammonium antibacterial agent, 2kg of ammonia water, 2kg of acrylic acid copolymer, 0.2kg of fatty alcohol polyoxyethylene ether (penetrant JFC), and 45.6kg of water.
[0047] Its preparation method comprises the following steps in turn:
[0048] (1) Mix acrylic latex, polyvinyl alcohol and water evenly;
[0049] (2) Under stirring conditions, add fatty alcohol polyoxyethylene ether, quaternary ammonium salt antibacterial agent, ammonia water, and acrylic acid copolymer in sequence, and mix evenly to obtain a sticky finishing agent. The stirring speed is 200r / min, and the stirring time is for 5min.
[0050] Further, the ...
Embodiment 2
[0052] A sticky finishing agent, the composition of which is as follows: the adhesive includes 68kg of acrylic latex (glass transition temperature is -38°C), 3kg of silver ion antibacterial agent, 0.1kg of ammonia water, 0.1kg of acrylic acid copolymer, fatty alcohol polyoxyethylene ether (Penetrant JFC) 0.5kg, water 28.3kg.
[0053] Its preparation method comprises the following steps in turn:
[0054] (1) Mix acrylic latex with water evenly;
[0055] (2) Under stirring conditions, add fatty alcohol polyoxyethylene ether, silver ion antibacterial agent, ammonia water, and acrylic acid copolymer in sequence, and mix evenly to obtain a sticky finishing agent. The stirring speed is 50r / min, and the stirring time is 15min.
[0056] Further, the sticky finishing agent was applied to the woven fabric by dipping, with a scrap rate of 95%, and product 2 was obtained after drying at 90°C.
Embodiment 3
[0058] A sticky finishing agent, its composition is as follows: polyurethane latex (glass transition temperature is -35 ℃) 80kg, quaternary ammonium salt antibacterial agent 1kg, ammonia water 0.2kg, polyurethane associative thickener 1.5kg, cationic polyammonium salt infiltration Agent 0.5kg, water 16.8kg.
[0059] Its preparation method comprises the following steps in turn:
[0060] (1) Mix polyurethane latex with water evenly;
[0061] (2) Under stirring conditions, sequentially add cationic polyammonium salt penetrating agent, quaternary ammonium salt antibacterial agent, ammonia water, and polyurethane associative thickener, and mix evenly to obtain a sticky finishing agent. The stirring speed is 100r / min, the stirring time is 10min.
[0062] Further, the sticky finishing agent was applied to the needle-punched non-woven fabric by dipping, with a scrap rate of 110%, and product 3 was obtained after drying at 80°C.
PUM
Property | Measurement | Unit |
---|---|---|
glass transition temperature | aaaaa | aaaaa |
glass transition temperature | aaaaa | aaaaa |
glass transition temperature | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com