A technology of chlorine dioxide mother liquor and chlorine dioxide, applied in botany equipment and methods, chemicals for biological control, animal repellants, etc., can solve the problems of chlorine dioxide instability and improve stability , prolong the release path, enhance the effect of sustained release
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Stir and mix 5 parts of graphene and 10 parts of alkylphenol polyoxyethylene ether evenly for later use; then add it to 75 parts of an aqueous solution containing 25% sodium chlorite and stir at high speed so that sodium chlorite enters the pores of graphene middle. Then add 20 parts of 20% aqueous solution containing sodium bisulfate to the above solution, and stir at room temperature for 2 hours, so that the chlorine dioxide mother liquor is fully reacted and intensified to generate chlorine dioxide molecules, which are fully adsorbed in the graphene pores. Then add one part per thousand of micro-nano silver and fully stir and disperse to form a chlorine dioxide slow-release solution.
Embodiment 2
[0020] Stir and mix 6 parts of molecular sieves and 15 parts of an aqueous solution containing 40% tetrabutylammonium bromide evenly and set aside; in the molecular sieve pores. Then add 25 parts of citric acid-containing 20% aqueous solution to the above solution, and stir at room temperature for 2 hours, so that the chlorine dioxide mother liquor is fully reacted and intensified to generate chlorine dioxide molecules, which are fully adsorbed in the molecular sieve pores. Then add 1 / 1000 part of micronano zinc and fully stir and disperse to form a chlorine dioxide slow-release solution.
Embodiment 3
[0022] 7 parts of activated carbon and 15 parts of sodium dodecylbenzenesulfonate aqueous solution containing 20% were stirred and mixed uniformly for later use; Barium chlorite enters the activated carbon pores. Then add 20 parts of 15% aqueous solution containing sodium dihydrogen phosphate to the above solution, and stir at room temperature for 2 hours, so that the chlorine dioxide mother liquor is fully reacted and intensified to generate chlorine dioxide molecules, which are fully adsorbed in the pores of the activated carbon. Then add 0.5 parts per thousand of micro-nano silver to fully stir and disperse to form a chlorine dioxide slow-release solution.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com