A technology for calcite and phosphate rock, applied in flotation, solid separation and other directions, can solve the problems of difficulty in separating high-grade phosphate concentrate, harsh process conditions, and low recovery rate of phosphate concentrate, and achieves enhanced floatability. Sexual differences, reduced surface coverage, the effect of a simple method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Embodiment 1, a pre-flotation treatment method for calcite-containing phosphate rock, the method is to add a surface treatment agent and an inhibitor to the calcite-containing phosphate rock slurry before flotation and slurry conditioning; the surface treatment agent For sulfuric acid or sulfurous acid or oxalic acid. The treatment was carried out with stirring, and the stirring time was 30 minutes. The addition amount of the surface treatment agent is 0.5kg / t raw ore. The inhibitor is a mixture of water glass, sodium fluoride and sodium lignosulfonate. The mass ratio of water glass, sodium fluoride and sodium lignosulfonate is 10:1:1.
Embodiment 2
[0019] Embodiment 2, a pre-flotation treatment method for calcite-containing phosphate rock, the method is to add a surface treatment agent and an inhibitor to the calcite-containing phosphate rock slurry before flotation and slurry adjustment; the surface treatment agent For sulfuric acid or sulfurous acid or oxalic acid. While processing, stirring was performed, and the stirring time was 120 minutes. The addition amount of the surface treatment agent is 10kg / t raw ore. The inhibitor is a mixture of water glass, sodium fluoride and sodium lignosulfonate. The mass ratio of water glass, sodium fluoride and sodium lignosulfonate was 10:4:3.
Embodiment 3
[0020] Embodiment 3, a flotation pretreatment method for calcite-containing phosphate rock, the method is to add a surface treatment agent and an inhibitor to the calcite-containing phosphate rock slurry before flotation and slurry adjustment; the surface treatment agent It is a combination of sulfuric acid and sulfurous acid, each of which accounts for half. The treatment was carried out with stirring, and the stirring time was 60 minutes. The addition amount of the surface treatment agent is 2kg / t raw ore. The inhibitor is a mixture of water glass, sodium fluoride and sodium lignosulfonate. The mass ratio of water glass, sodium fluoride and sodium lignosulfonate was 10:2:3.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com