Environment-friendly foam preparation and preparation method thereof
A foam and preparation technology, applied in the field of preparation of environmentally friendly foam preparations, can solve the problems of high cost and environmental pollution of environmentally friendly foam preparations, and achieve the effects of good foaming ability, good corrosion resistance and long shelf life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0022] The present invention also provides a kind of preparation method of environmental protection foam preparation, comprises the following steps:
[0023] Step 1, according to the weight ratio of 1:2:3:4, take respectively sodium α-methyl sulfopalmitate, modified silicone resin polyether emulsion, coconut oil fatty acid diethanolamide and methyl cellulose, and place In the flask, and stir at a speed of 100-200r / min until the mixture is uniform, and the foam stabilizer is obtained;
[0024] Step 2, weigh the following raw materials according to the weight ratio in decibels: sodium lauryl sulfate 5-15%, octylphenol polyoxyethylene ether 2-6%, alkylphenol polyoxyethylene ether 2-6%, methyl iso 0.2-2% thiazolinone, 0.2-1% sodium ethylenediamine tetramethylene phosphonate, 0.2-2% fatty acid diethanolamide, the balance is deionized water, and the water temperature is 30-40°C;
[0025] Step 3, stir and mix the raw materials weighed in step 2 at a speed of 50-100r / min, and slowly ...
Embodiment 1
[0027] Step 1, according to the weight ratio of 1:2:3:4, take respectively sodium α-methyl sulfopalmitate, modified silicone resin polyether emulsion, coconut oil fatty acid diethanolamide and methyl cellulose, and place In the flask, and stir at a speed of 10r / min until uniformly mixed to obtain a foam stabilizer;
[0028] Step 2, weigh the following raw materials according to the weight ratio in decibels: 5% sodium lauryl sulfate, 2% octylphenol polyoxyethylene ether, 2% alkylphenol polyoxyethylene ether, 0.2% methylisothiazolinone, Sodium ethylenediamine tetramethylene phosphonate 0.2%, fatty acid diethanolamide 0.2%, the balance is deionized water, and the water temperature is 30°C;
[0029] Step 3, stir and mix the raw materials weighed in step 2 at a speed of 50 r / min, and slowly add 4% of the foam stabilizer prepared in step 1 according to the weight ratio during the stirring process, and let stand for 20 minutes to obtain an environmentally friendly foam preparation. ...
Embodiment 2
[0031] Step 1, take by weight 1:2:3:4 sodium α-methyl sulfopalmitate, modified silicone resin polyether emulsion, coconut oil fatty acid diethanolamide and methyl cellulose respectively, and place In the flask, and stir at a speed of 200r / min until uniformly mixed to obtain a foam stabilizer;
[0032] Step 2, weigh the following raw materials according to the weight ratio in decibels: 15% sodium lauryl sulfate, 6% octylphenol polyoxyethylene ether, 6% alkylphenol polyoxyethylene ether, 2% methylisothiazolinone, Sodium ethylenediamine tetramethylene phosphonate 1%, fatty acid diethanolamide 2%, the balance is deionized water, and the water temperature is 40°C;
[0033] Step 3, stir and mix the raw materials weighed in step 2 at a speed of 100 r / min, and slowly add 10% of the foam stabilizer prepared in step 1 according to the weight ratio during the stirring process, and let stand for 50 minutes to obtain an environmentally friendly foam preparation.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com