A tobacco sheet and protective agent technology, which is applied in the fields of tobacco, tobacco processing, and tobacco preparation, can solve the problems of thin sheets and thin sheets without a good diaphragm, molecular motion adhesion, and large contact area, so as to achieve long retention time, reduce adhesion, The effect of enhancing the stability of film formation

Active Publication Date: 2022-04-08
HUBEI CHINA TOBACCO IND +1
View PDF19 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0003] At present, the problem of sticking in the storage of tobacco sheets in the production process of tobacco sheets is a major problem in the storage and use of tobacco sheets. Due to the large amount of tobacco sheet production, it generally needs to be stored for 2-3 months. The phenomenon of adhesion will occur during storage. There are two main reasons. One, a tobacco sheet is relatively flat, after extrusion, the contact area is large, and because the tobacco sheet has a high water content, it will stick after being placed for a long time. The second reason is that the tobacco sheet itself contains water, and there is no Very good diaphragm, molecular movement leads to adhesions

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • A method for preventing sticking of tobacco sheets
  • A method for preventing sticking of tobacco sheets
  • A method for preventing sticking of tobacco sheets

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0026] Preparation of water-soluble rosin pentaerythritol ester:

[0027] Weigh 300 g of refined rosin, grind it into a 500 mL four-neck flask, heat and melt it, when the temperature rises to about 160-170°C, stir, slowly add a certain amount of maleic anhydride, and keep it at about 185-190°C , react for 2 hours, add a certain amount of pentaerythritol and 0.3g of a common esterification catalyst, heat up to 210-250°C, react for 2-5h, remove moisture and low boiling point substances, cool down to about 200°C, and discharge to obtain water-soluble rosin pentaerythritol esters.

Embodiment 2

[0029] Preparation of anti-adhesive tobacco sheets:

[0030] Tobacco waste is manually cleaned, pretreated by washing stems, and dried;

[0031] Weigh 500g of the raw material after removal of impurities and put it into 2.5L extract solution, the extract solution is 2% urine solution aqueous solution, ultrasonic extraction at 40-60°C, the ultrasonic extraction frequency is 3KHz-5KHz, the extraction time is 4-6h, solid-liquid Extraction obtained after separation and treatment;

[0032] Centrifuge the extract with a butterfly centrifuge at 12000r / min, centrifuge for 3-5min, reduce the slag content, and take the supernatant;

[0033] Concentrate the purified extract to 40% using a double-effect rising film evaporator to obtain a concentrate;

[0034] Filter the concentrated solution through a 200-mesh rectangular sieve to obtain a filtered concentrated solution; according to the "Technical Specifications for Reconstituted Tobacco Leaf by Papermaking Method", add flavors and fra...

Embodiment 3

[0041] Preparation of anti-adhesive tobacco sheets:

[0042] Tobacco waste is manually cleaned, pretreated by washing stems, and dried;

[0043] Weigh 500g of the raw material after removal of impurities and put it into 2.5L extract solution, the extract solution is 2% urine solution aqueous solution, ultrasonic extraction at 40-60°C, the ultrasonic extraction frequency is 3KHz-5KHz, the extraction time is 4-6h, solid-liquid Extraction obtained after separation and treatment;

[0044] Centrifuge the extract with a butterfly centrifuge at 12000r / min, centrifuge for 3-5min, reduce the slag content, and take the supernatant;

[0045] Concentrate the purified extract to 40% using a double-effect rising film evaporator to obtain a concentrate;

[0046] Filter the concentrated solution through a 200-mesh rectangular sieve to obtain a filtered concentrated solution; according to the "Technical Specifications for Reconstituted Tobacco Leaf by Papermaking Method", add flavors and fra...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
thicknessaaaaaaaaaa
Login to View More

Abstract

A method for preventing sticking of tobacco sheets disclosed in the present invention comprises the following steps: spraying a protective agent on the tobacco sheets and drying them, shaping the tobacco sheets, reducing the contact area of ​​the sheets, increasing the pressure resistance elasticity of the sheets, and increasing the The film-forming properties between the sheets block the molecular movement of the contact surface of the tobacco sheets, and can also reduce the moisture content in the tobacco sheets to reduce adhesion.

Description

technical field [0001] The invention relates to the field of tobacco sheets, in particular to a method for preventing the storage of tobacco sheets from conglutination. Background technique [0002] Tobacco sheet is one of the important raw materials of cigarette products, which has a great impact on the quality of cigarette products. At the same time, it is also the main raw material of new heat-not-burn tobacco products. [0003] At present, the problem of sticking in the storage of tobacco sheets in the production process of tobacco sheets is a major problem in the storage and use of tobacco sheets. Due to the large amount of tobacco sheet production, it generally needs to be stored for 2-3 months. The phenomenon of adhesion will occur during storage. There are two main reasons. One, a tobacco sheet is relatively flat, after extrusion, the contact area is large, and because the tobacco sheet has a high water content, it will stick after being placed for a long time. The s...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
Patent Type & Authority Patents(China)
IPC IPC(8): A24B3/14A24B3/12A24B15/26
CPCA24B3/14A24B3/12A24B15/26
Inventor 童宇星李鹏飞喻世涛蒋心圆姚建武彭瑞王水明
Owner HUBEI CHINA TOBACCO IND
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Patsnap Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Patsnap Eureka Blog
Learn More
PatSnap group products