Blood vessel protection belt and preparation method and application thereof
A protective tape and blood vessel technology, applied in the field of medical devices, can solve the problems of increasing the burden on the liver, prolonging the degradation time, corrosion of blood vessel digestive juice, etc., and achieving the effects of convenient industrial production, simple production process and high product purity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0048] (Example 1, vascular protection tape and preparation method thereof)
[0049] The vascular protection tape of this embodiment is made of elongated collagen film, the chemical composition is completely composed of collagen, the width is 0.1cm1-2cm, and the thickness is 0.2-2mm. The length of the collagen fibers of the vascular protection zone or the greater the molecular weight of the collagen, the longer the degradation time in the body.
[0050] The preparation method of the above-mentioned vascular protection belt comprises the following steps:
[0051] ① Preparation of raw materials. Wash, clean and depilate cowhide (without mad cow disease) from a qualified slaughterhouse, and then use a piece of hide to remove the lower layer of flesh and upper epidermis to obtain a collagen fiber layer. Soak the fiber layer in 0.5% to 2% sodium carbonate solution, turn it constantly, and then dry it. The collagen fiber layer is added with acetone to degrease and air-dry several...
Embodiment 2
[0076] (Example 2, vascular protection tape and preparation method thereof)
[0077] The vascular protection tape of this embodiment is made of a strip-shaped collagen composite film, with a width of 0.1cm1-2cm and a thickness of 0.2-2mm.
[0078] The components and their mass percentages in the collagen composite film are as follows: 60% to 90% of collagen, 10% to 40% of degradable biopolysaccharides, wherein the degradable biopolysaccharides are sodium hyaluronate, cross-linked transparent One or more of sodium alginate, chitosan, dextran, and bacterial cellulose.
[0079] The biopolysaccharide in this example is composed of modified sodium hyaluronate and cross-linked sodium hyaluronate with a mass ratio of 1:1.
[0080] The modification method of sodium hyaluronate is: dissolve medical grade hyaluronic acid in water, carry out oxidation reaction with excess sodium periodate solution, add sodium bisulfite solution after the reaction to reduce unreacted residual oxidant, wa...
Embodiment 3
[0084] (Embodiment 3, blood vessel protection band)
[0085] The components and their mass percentages in the vascular protection tape of this embodiment are as follows: 75% collagen and 25% bacterial cellulose.
PUM
Property | Measurement | Unit |
---|---|---|
Width | aaaaa | aaaaa |
Thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com