Embodiment 1
[0031] Such as figure 1 As shown, it includes the outer steel body 1, the inner thermoplastic body 2 and the reinforced plastic sleeve 3. In the structural design of the entire pipe fitting, the outer steel body 1 plays the role of bearing the hoop stress, and the inner thermoplastic body 2 plays the role of bearing Anti-corrosion effect, the reinforced plastic sleeve 3 plays the role of anti-axial stress.
[0032] Wherein the outer casing steel body 1 includes the receiving section 11 located at both ends and the transfer section 12 located in the middle, the connection between the two ends of the transfer section 12 and the corresponding receiving section 11 is formed as a whole by external electric welding, and the port of the receiving section 11 There are several equidistant bolt holes in the circumferential direction, and the transition section 12 can be an elbow, a tee, a direct connection, a flange, etc., and the lining thermoplastic body 2 includes a liner thermoplast...
Embodiment 2
[0034] The invention also discloses a method for manufacturing a steel-lined plastic-coated anti-corrosion and high-pressure resistant pipe fitting, which includes the following steps:
[0035] A1. Select the receiving section 11 whose inner diameter is 8mm to 20mm larger than the outer diameter of the external composite pipe, and the wall thickness of the receiving section 11 should be 8mm larger than the diameter of the tie bolt;
[0036] A2. Select the transfer section 12 whose nominal diameter is equal to the inner diameter of the external composite pipe, weld and fix the root of the finished product of the receiving section 11 and the port of the transfer section 12 to form the outer steel body 1;
[0037] A3. Heat the jacket steel body 1 to 250°C-400°C as a whole, keep the jacket steel body at 200°C-250°C with built-in thermoplastic powder coating plastic melt, and after natural cooling and shaping to obtain the lining thermoplastic body 2, remove The remaining thermopla...
PUM
Property | Measurement | Unit |
---|---|---|
thickness | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com