High-performance adsorbent formula of electroplating waste water
A technology for electroplating wastewater and adsorbent, which is used in metallurgical wastewater treatment, adsorption water/sewage treatment, water pollutants and other directions to achieve high adsorption efficiency, improve adsorption stability, and good adsorption effect.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] A high-efficiency adsorbent formula for electroplating wastewater. The raw materials of the adsorbent include the following components in parts by weight: 22 parts of sulfonated coal, 15 parts of semi-coke, 25 parts of lipase liquid, 5 parts of sodium humate, and nano-ferric oxide 15 parts, 15 parts of sodium carboxymethyl starch, 5 parts of polyaluminum chloride, 10 parts of bamboo charcoal powder, 3 parts of polyacrylamide, 8 parts of polyaspartic acid, 6 parts of polyvinyl butyral, 5 parts of chitosan 4 parts, 7 parts of 45% H2O2, 6 parts of acrylic polymer water-absorbing resin, 4 parts of maleic anhydride grafted polypropylene, 2 parts of PET, 5 parts of hydroxyethyl methacrylate, 4 parts of phosphorus molybdenum phenolic resin powder, high wear-resistant carbon 1 part black, 4 parts hydroxycellulose solution.
Embodiment 2
[0012] High-efficiency adsorbent formula for electroplating wastewater. The raw materials of the adsorbent include the following components by weight: 23 parts of sulfonated coal, 18 parts of semi-coke, 27 parts of lipase liquid, 7 parts of sodium humate, and 16 parts of nano-ferric oxide , 17 parts of sodium carboxymethyl starch, 7 parts of polyaluminum chloride, 11 parts of bamboo charcoal powder, 4 parts of polyacrylamide, 11 parts of polyaspartic acid, 8 parts of polyvinyl butyral, 6 parts of chitosan, 9 parts of 45% H2O2, 8 parts of acrylic polymer water-absorbing resin, 7 parts of maleic anhydride grafted polypropylene, 4 parts of PET, 7 parts of hydroxyethyl methacrylate, 7 parts of phosphorus molybdenum phenolic resin powder, and 2 parts of high wear-resistant carbon black Parts, 6 parts of hydroxycellulose solution.
Embodiment 3
[0014] High-efficiency adsorbent formula for electroplating wastewater. The raw materials of the adsorbent include the following components by weight: 25 parts of sulfonated coal, 20 parts of semi-coke, 30 parts of lipase solution, 8 parts of sodium humate, and 18 parts of nano-ferric oxide , 18 parts of sodium carboxymethyl starch, 8 parts of polyaluminum chloride, 12 parts of bamboo charcoal powder, 5 parts of polyacrylamide, 14 parts of polyaspartic acid, 11 parts of polyvinyl butyral, 8 parts of chitosan, 10 parts of 45% H2O2, 11 parts of acrylic polymer water-absorbing resin, 10 parts of maleic anhydride grafted polypropylene, 6 parts of PET, 8 parts of hydroxyethyl methacrylate, 10 parts of phosphorus molybdenum phenolic resin powder, 3 parts of high wear-resistant carbon black Parts, 9 parts of hydroxycellulose solution.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com