A compound additive for reducing phenol release in flue gas and its application
A technology for compounding additives and releasing amount, applied in application, tobacco, e-liquid filter and other directions, can solve the problems of inability to effectively remove harmful substances, inability to reduce phenol content, complicated preparation process, etc., and achieve obvious harm reduction effect and low cost. , the preparation method is simple
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0021] A clear and complete description will be made below in conjunction with the technical solutions in the embodiments. Apparently, the described embodiments are only some examples of the present invention, not all examples. Based on the embodiments of the present invention, all other embodiments obtained by persons of ordinary skill in the art without making creative efforts belong to the protection scope of the present invention.
[0022] Example 1
[0023] The polyvinylpyrrolidone compound additive for reducing phenol release in smoke involved in this example includes the following raw materials in parts by weight: 5 parts of polyvinylpyrrolidone, 2 parts of acid compounds, 2 parts of polyols and 20 parts of solvent.
[0024] The preparation method of the compound additive for reducing the amount of phenol released in the flue gas involved in this embodiment is carried out as follows:
[0025] Add 2g of citric acid and 2g of polyvinyl alcohol into 20g of water, stir for...
Embodiment 2
[0034] The polyvinylpyrrolidone compound additive for reducing phenol release in smoke involved in this example includes the following raw materials in parts by weight: 1 part of polyvinylpyrrolidone, 0.1 part of acid compound, 0.1 part of polyol and 40 parts of solvent.
[0035] The preparation method of the compound additive for reducing the amount of phenol released in the flue gas involved in this embodiment is carried out as follows:
[0036] Add 0.02g of oxalic acid and 0.08g of glycine, 0.05g of ethylene glycol and 0.05g of propylene glycol into 50g of ethanol, stir for 5 minutes to obtain a uniform solution, then add 1g of polyvinylpyrrolidone with a molecular weight of 1,000,000, and stir for 5 minutes to obtain a uniform solution. compound additive products.
[0037] The compound additives are added according to 1% of the tow weight in each nozzle rod.
[0038] The smoke components of the prepared cigarettes were analyzed, and the blank sample was a cigarette withou...
Embodiment 3
[0042] The polyvinylpyrrolidone compound additive for reducing phenol release in smoke involved in this example includes the following raw materials in parts by weight: 20 parts of polyvinylpyrrolidone, 5 parts of acid compounds, 5 parts of polyols and 50 parts of solvent.
[0043] The preparation method of the compound additive for reducing the amount of phenol released in the flue gas involved in this embodiment is carried out as follows:
[0044] Add 0.5g of alanine, 4.5g of tartaric acid and 5g of glycerin into 50g of water, stir for 7min to obtain a uniform solution, then add 10g of polyvinylpyrrolidone with a molecular weight of 400,000 and 10g of vinylpyrrolidone-maleic acid copolymer, and stir for 10min Even, it is the required compound additive product.
[0045] Composite additives are added by 3% of the tow weight in each nozzle rod.
[0046] The smoke components of the prepared cigarettes were analyzed, and the blank sample was a cigarette without any materials add...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com