Embodiment 1
[0074] Add 18 parts of bisphenol S, 17 parts of sodium phenolsulfonate, 1 part of potassium hydroxide and 48 parts of deionized water into a reaction device with a stirrer and a condenser, heat up to 85°C, and add 12 parts of formaldehyde solution dropwise , the rate of addition is 20ml / min. After the dropwise addition is completed within 1 hour, the temperature is raised to boiling, and the heat preservation and reflux reaction is carried out for 10 hours; MPa) to react for 0.5 hour, lower the temperature to 80° C.; then add 0.8 parts of polyepoxysuccinic acid and 3 parts of sodium p-toluenesulfonate, stir for 0.5 hour, and obtain a synthetic tannin color fixing agent after cooling. The solid content of the color fixing agent is about 43%.
[0075] The mass percentages of the various raw materials of the color-fixing agent in Example 1 are: 18% of phenolic compounds, 17% of aromatic sulfonic acid compounds, 1% of catalyst, 12% of formaldehyde solution, 0.6% of modifying agent...
Embodiment 2
[0077] Add 15 parts of sulfonated bisphenol S, 10 parts of phenol sulfonic acid, 10 parts of naphthol sulfonic acid, 5 parts of sodium hydroxide, 2 parts of ethylenediamine di-o-phenylacetic acid and 39 parts of deionized water with a stirrer and In the reaction device of the condenser, heat up to 90°C, add 15 parts of formaldehyde solution dropwise, and the drop rate is 15ml / min. After the dropwise addition is completed within 2 hours, heat up to boiling, keep warm and reflux for 6 hours; then add 2 1 part of sodium thiosulfate, continue to keep warm for 1.5 hours, then vacuumize (vacuum degree is 0.05-0.1MPa) for 1 hour, cool down to 60 ° C; add 2 parts of sodium p-dodecyl diphenyl ether disulfonate, After stirring for 0.5 hour, the synthetic tannin color fixing agent is obtained after cooling. The color fixing agent has a solid content of about 45%.
[0078] The mass percentages of each raw material of the color-fixing agent in Example 2 are: 15% of phenolic compound, 20% ...
Embodiment 3
[0080] Add 15 parts of bisphenol S, 5 parts of phenol, 16 parts of naphthalenesulfonic acid, 3 parts of potassium hydroxide, 1.5 parts of ethylenediamine di-o-phenylacetic acid, 1 part of sodium xylenesulfonate and 48 parts of deionized water with In the reaction device of the agitator and condenser, heat up to 95°C, add 10 parts of formaldehyde solution dropwise at a rate of 15ml / min, after the dropwise addition is completed within 1.5 hours, heat up to boiling, and keep warm for reflux for 7 hours; then Then add 1 part of sodium bisulfite, continue the heat preservation reaction for 0.5 hours, then vacuumize (0.05-0.1 MPa) and react for 1 hour, after cooling down, the synthetic tannin color fixing agent is obtained. The solid content of the color fixing agent is about 44%.
[0081] The mass percent of each raw material of color fixing agent in embodiment 3 is: phenolic compound 20%, aromatic sulfonic acid compound 16%, catalyst 3%, formaldehyde solution 10%, modifier 1%, che...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com