Cement water-reducing agent and preparation method thereof
A water-reducing agent and cement technology, applied in the chemical industry, can solve the problems of poor water-reducing dispersing ability and slump-preserving effect of the water-reducing agent, and achieve the effect of strong dispersion and water reduction, moderate molecular weight, and surface tension reduction.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0026]Sieve particles: Take calcium lignosulfonate and add distilled water at a mass ratio of 1:2 to stir and mix, then add 10% of calcium lignosulfonate to sulfuric acid with a mass fraction of 10% and mix, and stir and mix at 35°C for 40 minutes to obtain a mixture Mixture, take the stirred mixture according to the mass ratio of 10:3:1, add hydrogen peroxide and sodium bisulfite with a mass fraction of 30%, mix, heat up to 75°C, stir and mix for 3 hours, centrifuge, and take the supernatant according to the mass ratio of 1:8 Add absolute ethanol for mixing, filter, take the precipitate, grind and pulverize it through a 100-mesh sieve, and collect the sieved particles.
[0027] Wenlun rubber: purchased from Shanghai Shunshui Chemical Co., Ltd.
[0028] Water reducer base material: (1) In parts by mass, take 20 parts of isopentenol polyoxyethylene ether, 5 parts of butyl acrylate, 70 parts of deionized water, 5 parts of hydrogen peroxide with a mass fraction of 10%, 12 1 part...
Embodiment 2
[0034] Sieve particles: Take calcium lignosulfonate and add distilled water at a mass ratio of 1:2 to stir and mix, then add 20% of the mass of calcium lignosulfonate to sulfuric acid with a mass fraction of 10% and mix, stir and mix at 45°C for 50 minutes to obtain Mixture, take the stirred mixture according to the mass ratio of 10:3:1, add hydrogen peroxide and sodium bisulfite with a mass fraction of 30%, mix, heat up to 85°C, stir and mix for 4 hours, centrifuge, and take the supernatant according to the mass ratio of 1:8 Add absolute ethanol for mixing, filter, take the precipitate, grind and pulverize it through a 100-mesh sieve, and collect the sieved particles.
[0035] Wenlun rubber: purchased from Shanghai Shunshui Chemical Co., Ltd.
[0036] Water reducer base material: (1) In parts by mass, take 30 parts of isopentenol polyoxyethylene ether, 8 parts of butyl acrylate, 90 parts of deionized water, 9 parts of hydrogen peroxide with a mass fraction of 10%, 15 parts 1...
Embodiment 3
[0042] Sieve particles: Take calcium lignosulfonate and add distilled water at a mass ratio of 1:2 to stir and mix, then add 15% of calcium lignosulfonate to sulfuric acid with a mass fraction of 10% and mix, stir and mix at 40°C for 45 minutes to obtain a mixture Mixture, take the stirred mixture according to the mass ratio of 10:3:1, add hydrogen peroxide and sodium bisulfite with a mass fraction of 30%, mix, heat up to 80°C, stir and mix for 3 hours, centrifuge, and take the supernatant according to the mass ratio of 1:8 Add absolute ethanol for mixing, filter, take the precipitate, grind and pulverize it through a 100-mesh sieve, and collect the sieved particles.
[0043] Wenlun rubber: purchased from Shanghai Shunshui Chemical Co., Ltd.
[0044] Water reducer base material: (1) In parts by mass, take 25 parts of isopentenol polyoxyethylene ether, 7 parts of butyl acrylate, 80 parts of deionized water, 7 parts of hydrogen peroxide with a mass fraction of 10%, 13 1 part of...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com