Environment-friendly water-based fire extinguishing agent
A kind of fire extinguishing agent and environment-friendly technology, applied in the field of environment-friendly water-based fire extinguishing agents, can solve the problems of inflow, pollution, seepage into the ground, etc., and achieve the effects of improving spray performance, reducing usage, and reducing waste
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0020] (1) Preparation of inorganic salts
[0021] It is prepared by mixing 10 parts by mass of ammonium hydrogen phosphate, 15 parts of ammonium dihydrogen phosphate, 8 parts of phosphobenzoic acid, 1 part of calcium hydroxide and 20 parts of water.
[0022] (2) Preparation of antifreeze
[0023] Mix 12 parts of polyethylene glycol, 6 parts of polyvinyl alcohol, 6 parts of glycerin, and 40 parts of water, and then perform high-speed stirring for 2 hours to obtain an emulsion.
[0024] (3) Preparation of stabilizer
[0025] Mix 12 parts of urea, 1 part of sodium bisulfite, 2 parts of sodium dodecylsulfonate, and 25 parts of water to obtain a product after mixing evenly.
[0026] (4) Preparation of hydrocarbon surfactant
[0027] A substance prepared by mixing 20 parts of amphoteric imidazoline with 18 carbon atoms, 10 parts of betaine, and 2 parts of sodium stearate at 70°C with 35 parts of water.
[0028] (5) Preparation of thermosensitive hydrogel
[0029] 12 parts by m...
Embodiment 2
[0033] (1) Preparation of inorganic salts
[0034] It is prepared by mixing 15 parts by mass of ammonium hydrogen phosphate, 18 parts of ammonium dihydrogen phosphate, 7 parts of phosphobenzoic acid, 1 part of calcium hydroxide and 25 parts of water.
[0035] (2) Preparation of antifreeze
[0036] 15 parts of polyethylene glycol, 6 parts of polyvinyl alcohol, 10 parts of glycerin, and 50 parts of water were mixed, and then stirred at a high speed for 3 hours to obtain an emulsion.
[0037] (3) Preparation of stabilizer
[0038] Mix 15 parts of urea, 2 parts of sodium bisulfite, 2 parts of sodium dodecylsulfonate, and 25 parts of water to obtain a product after mixing evenly.
[0039] (4) Preparation of hydrocarbon surfactant
[0040] A substance prepared by mixing 25 parts of amphoteric imidazolines with 15 carbon atoms, 15 parts of betaine, and 4 parts of sodium stearate at 75°C with 40 parts of water.
[0041] (5) Preparation of thermosensitive hydrogel
[0042] 15 part...
Embodiment 3
[0046] (1) Preparation of inorganic salts
[0047]It is prepared by mixing 20 parts by mass of ammonium hydrogen phosphate, 20 parts of ammonium dihydrogen phosphate, 6 parts of phosphobenzoic acid, 1 part of calcium hydroxide and 20 parts of water.
[0048] (2) Preparation of antifreeze
[0049] 10 parts of polyethylene glycol, 6 parts of polyvinyl alcohol, 6 parts of glycerin, and 40 parts of water were mixed, and then stirred at a high speed for 2 hours to obtain an emulsion.
[0050] (3) Preparation of stabilizer
[0051] Mix 12 parts of urea, 2 parts of sodium bisulfite, 2 parts of sodium dodecylsulfonate, and 22 parts of water, and mix them uniformly to obtain a product.
[0052] (4) Preparation of hydrocarbon surfactant
[0053] A substance prepared by mixing 20 parts of amphoteric imidazolines with 12 carbon atoms, 10 parts of betaine, and 6 parts of sodium stearate at 70°C with 30 parts of water.
[0054] (5) Preparation of thermosensitive hydrogel
[0055] The m...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com