A drainage asphalt and durability technology, applied in building thermal insulation materials, building components, buildings, etc., can solve problems such as stone loss, drainage asphalt pavement damage, shortening the service life of pavement, etc., and achieve increased thickness, local or overall enhancement. , The effect of improving the anti-scattering ability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] Example 1 An anti-scattering material for durable drainage asphalt pavement
[0033] This embodiment provides an anti-scattering material for durable drainage asphalt pavement, which is composed of water-based epoxy resin emulsion, modified emulsified asphalt, and water in a weight ratio of 2.5:100:2.5.
[0034] Wherein, the water-based epoxy resin emulsion is obtained by mixing water-based epoxy resin and water-based epoxy resin curing agent with a weight ratio of 1:1.5, wherein the water-based epoxy resin is a water-soluble epoxy resin with a solid content of 80%. The oxygen value is 0.41; the water-based epoxy resin curing agent is tetraethylenepentamine, and its solid content is 50%.
[0035] The modified emulsified asphalt is a fast-cracking SBR modified emulsified asphalt with a solid content of 70%.
Embodiment 2
[0037] An anti-scattering material for durable drainage asphalt pavement provided in this embodiment is composed of water-based epoxy resin emulsion, modified emulsified asphalt, and water in a weight ratio of 2.5:100:5.0.
[0038] Wherein, the water-based epoxy resin emulsion is obtained by mixing water-based epoxy resin and water-based epoxy resin curing agent with a weight ratio of 1:1.5, wherein the water-based epoxy resin is a water-soluble epoxy resin with a solid content of 80%. The oxygen value is 0.41; the water-based epoxy resin curing agent is tetraethylenepentamine, and its solid content is 30%.
[0039] The modified emulsified asphalt is a fast-cracking SBR modified emulsified asphalt with a solid content of 70%.
Embodiment 3
[0041] An anti-scattering material for durable drainage asphalt pavement provided in this embodiment is composed of water-based epoxy resin emulsion, modified emulsified asphalt, and water in a weight ratio of 2.5:75:2.5.
[0042] The water-based epoxy resin emulsion is obtained by mixing water-based epoxy resin and water-based epoxy resin curing agent at a weight ratio of 1:1.5, wherein the water-based epoxy resin is a water-soluble epoxy resin with a solid content of 80% and an epoxy value of is 0.41; the water-based epoxy resin curing agent is triethylenetetramine, and its solid content is 50%.
[0043] The modified emulsified asphalt is fast-cracking SBR modified emulsified asphalt with a solid content of 75%.
PUM
Property | Measurement | Unit |
---|---|---|
epoxy value | aaaaa | aaaaa |
epoxy value | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com