High-toughness plastic barbell plate
A high-toughness, plastic technology, applied in the field of fitness equipment, can solve the problems of personal injury, increase bone density, insufficient toughness, etc., and achieve the effect of high yield, excellent performance and low price
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] The high-toughness plastic barbell of the present invention is made of the following components according to the weight fraction ratio:
[0011] Proportion by weight fraction is made from the following components:
[0012] 23 parts of SEBS, 6 parts of zinc oxide, 32 parts of PP, 5 parts of latex powder, 4 parts of zinc stearate, 2 parts of lauryl alcohol, 6 parts of polyphenylene sulfide, 12 parts of low-pressure polyethylene, dihydroxyalkyl phosphine 4 parts of tetraerythritol ester, 14 parts of tetraerythritol ester, 5 parts of phthalic anhydride, 23 parts of filler, 6 parts of zinc oxide, 7 parts of calcium carbonate, 4 parts of melamine cyanurate, 2 parts of calcium stearate, white carbon 3 parts of black, 5 parts of dioctyl phthalate, 33 parts of high pressure polyethylene, 23 parts of polyethylene resin, 21 parts of polyethylene resin, 9 parts of nano silicon dioxide, 6 parts of tribasic lead sulfate, alkylbenzene 4 parts of sulfonate, 12 parts of triphenyl phosp...
Embodiment 2
[0014] The high-toughness plastic barbell of the present invention is made of the following components according to the weight fraction ratio:
[0015] Proportion by weight fraction is made from the following components:
[0016] 27 parts of SEBS, 9 parts of zinc oxide, 38 parts of PP, 8 parts of latex powder, 7 parts of zinc stearate, 5 parts of lauryl alcohol, 12 parts of polyphenylene sulfide, 23 parts of low-pressure polyethylene, dihydroxyalkyl phosphine 9 parts of acid salt, 17 parts of tetraerythritol ester, 8 parts of phthalic anhydride, 25 parts of filler, 6 parts of zinc oxide, 8 parts of calcium carbonate, 7 parts of melamine cyanurate, 2 parts of calcium stearate, white carbon 6 parts of black, 7 parts of dioctyl phthalate, 36 parts of high pressure polyethylene, 45 parts of polyethylene resin, 32 parts of polyethylene resin, 11 parts of nano silicon dioxide, 9 parts of tribasic lead sulfate, alkylbenzene 8 parts of sulfonate, 16 parts of triphenyl phosphate.
Embodiment 3
[0018] The high-toughness plastic barbell of the present invention is made of the following components according to the weight fraction ratio:
[0019] Proportion by weight fraction is made from the following components:
[0020] 25 parts of SEBS, 7 parts of zinc oxide, 35 parts of PP, 7 parts of latex powder, 5 parts of zinc stearate, 3 parts of lauryl alcohol, 9 parts of polyphenylene sulfide, 18 parts of low-pressure polyethylene, dihydroxyalkyl phosphine 7 parts of acid salt, 15 parts of tetraerythritol ester, 7 parts of phthalic anhydride, 24 parts of filler, 6 parts of zinc oxide, 7 parts of calcium carbonate, 5 parts of melamine cyanurate, 2 parts of calcium stearate, white carbon 4 parts of black, 6 parts of dioctyl phthalate, 35 parts of high pressure polyethylene, 32 parts of polyethylene resin, 27 parts of polyethylene resin, 10 parts of nano silicon dioxide, 7 parts of tribasic lead sulfate, alkylbenzene 6 parts of sulfonate, 14 parts of triphenyl phosphate.
[0...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com