A kind of environmentally friendly paper, a new technology, applied in the field of paper manufacturing, can solve the problems of affecting office efficiency, insufficient high temperature resistance, waste of resources, etc., and achieve the effect of improving office efficiency, high hardness and low cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] A preparation method of a novel environment-friendly paper, comprising the following preparation methods:
[0024] 1. Add the dry inorganic powder and the surface treatment agent into a high-speed mixer, and stir for 40 minutes at a temperature of 300°C to obtain a modified inorganic powder;
[0025] 2. Mix the modified inorganic powder and the high-temperature-resistant polymer evenly, then put them into the internal mixer, melt and blend for 2 hours, and then extrude and granulate through single-screw to obtain mixed pellets;
[0026] 3. Mix the mixed pellets, chain extender, heat stabilizer and foaming agent together, and sequentially undergo twin-screw melt extrusion and blow molding to obtain a thickness of 4mm to obtain a semi-finished product;
[0027] 4. Leave the semi-finished product at room temperature for 2 days to get the finished product.
[0028] The new environmentally friendly paper includes the following raw materials by weight: 50 parts of inorganic ...
Embodiment 2
[0036] A preparation method of a novel environment-friendly paper, comprising the following preparation methods:
[0037] 1. Add the dry inorganic powder and the surface treatment agent into a high-speed mixer, and stir for 40 minutes at a temperature of 300°C to obtain a modified inorganic powder;
[0038] 2. Mix the modified inorganic powder and the high-temperature-resistant polymer evenly, then add them into the internal mixer, melt and blend for 3 hours, and then obtain the mixed pellets through single-screw extrusion and granulation;
[0039] 3. Mix the mixed pellets, chain extender, heat stabilizer and foaming agent together, and sequentially undergo twin-screw melt extrusion and blow molding to obtain a thickness of 4mm to obtain a semi-finished product;
[0040] 4. Leave the semi-finished product at room temperature for 2 days to get the finished product.
[0041] The new environmentally friendly paper includes the following raw materials by weight: 40 parts of inorg...
PUM
Property | Measurement | Unit |
---|---|---|
particle size (mesh) | aaaaa | aaaaa |
particle size (mesh) | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com