A shield tail sealing and grease technology, which is applied in the oil/fat refining, fat production, petroleum industry, etc., can solve the problems of poor sealing performance of shield sealing grease, lack of solutions, and large amount of grease, etc., and achieves low cost and reduced cost. The effect of production cost and usage reduction
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0058] The components of shield tail seal grease are: 150kg of deep-processed waste oil, 10kg of agar, 40kg of gum arabic, 8kg of antifungal agent, 5kg of lubricant, 400kg of light calcium carbonate powder, and 38kg of bamboo fiber.
[0059] Preparation method: After mixing the deep-processed waste oil and bamboo fiber, stir for 20 minutes, then add 10kg of agar, 40kg of gum arabic, antifungal agent and lubricating oil to it, stir for 20 minutes, then add light calcium carbonate powder in batches during the stirring process (A small amount of continuous addition is required when adding), stirring for no less than 76 minutes until a uniform yellow viscous mixture is obtained.
Embodiment 2
[0061] The components of shield tail seal grease are: 130kg of deep-processed waste oil, 15kg of carrageenan, 45kg of agar, 12kg of antifungal agent, 6kg of lubricant, 330kg of mica powder, and 42kg of bamboo fiber.
[0062] Preparation method: After mixing the deep-processed waste oil and bamboo fiber, stir for 20 minutes, then add carrageenan, agar, anti-fungal agent and lubricating oil therein, after stirring for 20 minutes, add mica powder in batches during the stirring process (a small amount is required when adding Continuous addition), stirring for no less than 70 minutes, until a uniform yellow viscous mixture is obtained.
Embodiment 3
[0064] The components of shield tail seal grease are: 130kg of deep-processed waste oil, 15kg of alginic acid, 45kg of agar, 12kg of antifungal agent, 6kg of lubricant, 130kg of mica powder, 200kg of light calcium carbonate powder, and 42kg of bamboo fiber.
[0065] Preparation method: After mixing deep-process waste oil and bamboo fiber, stir for 15 minutes, then add alginic acid, agar, anti-fungal agent and lubricating oil to it, after stirring for 20 minutes, add mica powder and light calcium carbonate in batches during the stirring process powder (a small amount of continuous addition is required when adding), stirring for no less than 70 minutes until a uniform yellow viscous mixture is obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com