A production method and slag technology, which are applied in chemical instruments and methods, ceramic molding workshops, mixing plants, etc., can solve the problems of high cost of building mechanics, heavy unit volume of masonry, and large amount of steel, and achieve simple and fast production. , Low production cost, good processing performance
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment 1
[0045] 4mm ordinary calcium silicate decorative board is used as the panel, and the intermediate filler is a hydraulic substance. The formula of the hydraulic substance is: 10% gypsum powder, 20% slag (with a particle size below 15mm) , yellow sand 15%, 425# cement 55% to form a dry mix.
[0046] Each ton of dry mix is equipped with 2.5m 3 polystyrene particles.
[0047] Add water 24%, and various additives at 2.0%.
[0048] The 2.0% various additives are calculated per ton of dry mix: 2.0kg of hydroxypropyl methylcellulose, 0.7kg of dispersible latex powder, 12kg of early strength agent, 700ml of water reducing agent, and 1400ml of air-entraining agent.
[0049] The slag is crushed with a crusher, and the maximum particle size is required to be below 20 mm; it is light in weight and has a certain strength, and it is used as aggregate to make the particle product mix reach an ideal ratio.
specific Embodiment 2
[0051] Use a 5 mm ordinary calcium silicate decorative board as a panel, and the intermediate filler is a hydraulic substance. The formula of the hydraulic substance is: 15% gypsum powder, 25% slag (with a particle size below 15mm) , yellow sand 10%, 425# cement 50% to form a dry mix.
[0052] Each ton of dry mix is equipped with 2. 3m 3 polystyrene particles.
[0053] Add water 23%, and 1.5% of various additives.
[0054] The 1.5% of various additives is calculated per ton of dry mix: 1.6kg of hydroxypropyl methylcellulose, 0.7kg of dispersible latex powder, 10.5kg of early strength agent, 500ml of water reducing agent, and 1200ml of air-entraining agent wet mix.
[0055] The slag 2 is crushed with a crusher, and the maximum particle size is required to be below 20 mm; it is light in weight and has a certain strength, and is used as aggregate to make the particle product mix reach an ideal ratio.
[0056] Referring to the accompanying drawings, the outlets of the gypsum...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com