Method for microbial ash removal of coal
A microbial and coal technology, applied in the field of coal microbial deashing, can solve the problem of difficult removal of ash from coal slime, and achieve the effects of good deashing effect, extensive culture conditions and mild treatment conditions.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] The coal sample with an ash content of 40.85% is difficult to dissociate monomers due to the association of coal with the minerals that make up the ash content.
[0025] The concrete steps that adopt the present invention to carry out microbial deashing are as follows:
[0026] (1) The coal sample is crushed to less than 0.074mm;
[0027] (2) Preparation of liquid medium (sucrose 5.0 g / L, Na 2 HPO 4 2.0 g / L, MgSO 4 •7H 2 O 1.0 g / L, FeCl 3 0.01 g / L, CaCl 2 0.1 g / L, kaolin 0.5 g / L), add pulverized coal samples to the liquid medium, make a coal slurry with a mass concentration of 10%, adjust the pH value to 7.3, and sterilize by high-pressure steam;
[0028] (3) Introduce the Paenibacillus polymyxa into the coal slurry in step (2), the inoculated amount is 10% of the volume of the culture medium, and cultivate it in a constant temperature shaking incubator at 30°C, and the speed of the shaking incubator is 150 r / min, The deashing time is 7d;
[0029] (4) Deashed...
Embodiment 2
[0032] The ash content is 30.24% of coal slime, the particle size less than 0.045mm accounts for 51.38%, and the ash content of this particle size is 42.92%. The gangue minerals are mainly kaolin, illite and quartz.
[0033] The concrete steps that adopt the present invention to carry out microbial deashing are as follows:
[0034] (1) The coal sample is crushed to less than 0.074mm;
[0035] (2) Preparation of liquid medium (sucrose 2.0 g / L, Na 2 HPO 4 1.0 g / L, MgSO 4 •7H 2 O 0.5 g / L, FeCl 3 0.005 g / L, CaCl 2 0.15 g / L, add pulverized coal samples into the liquid medium, make a coal slurry with a concentration of 20%, adjust the pH value to 7.5, and sterilize by high-pressure steam;
[0036] (3) Inject 15% Paenibacillus polymyxa into the coal slurry in step (2), cultivate in a constant temperature shaking incubator at 28°C, the rotating speed of the shaking incubator is 200 r / min, and the deashing time is 4 days;
[0037] (4) Deashed coal was filtered, washed three t...
Embodiment 3
[0040] The ash content is 9.03% lignite clean coal, and the ash content is kaolin and quartz.
[0041] The concrete steps that adopt the present invention to carry out microbial deashing are as follows:
[0042] (1) The coal sample is crushed to less than 0.074mm;
[0043] (2) Preparation of liquid medium (Na 2 HPO 4 2.0 g / L, MgSO 4 •7H 2 O 0.75 g / L, FeCl 3 0.01 g / L, CaCl 2 0.1 g / L, kaolin 0.6 g / L), add pulverized coal samples to the liquid medium, make a coal slurry with a concentration of 15%, adjust the pH value to 7.0, and sterilize by high-pressure steam;
[0044] (3) Inject 20% of Paenibacillus polymyxa into the coal slurry in step (2), cultivate in a constant temperature shaking incubator at 30°C, the rotating speed of the shaking incubator is 180 r / min, and the deashing time is 3 days;
[0045] (4) Deashed coal was filtered, washed 5 times with water, and dried at 75°C for analysis.
[0046] The test results of this embodiment are: the clean coal yield is 92...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology