Embodiment 1
[0030] A biochar-based helical magnetic biofilm reactor composed of such as figure 1 The spiral U-shaped groove track shown is composed of magnetic bio-carbon filler loaded in the spiral U-shaped groove track; the spiral U-shaped groove track is ascending, and the plane of the spiral U-shaped groove track is The angle with the horizontal plane is 8 °, and the periphery of the spiral U-shaped groove track projected on the horizontal plane is circular, and the diameter of the circle is 4 times the width of the spiral U-shaped groove track. The length to width ratio of the groove track is 21, and the depth is 8cm; the material of the spiral U-shaped groove track is plexiglass.
[0031] Wherein the preparation method of magnetic bio-carbon filler is:
[0032] (1) Add excessive waste iron scraps to the waste liquid containing sulfuric acid, add biochar after reacting for 21 minutes, stir for 10 minutes, absorb ferrous ions in the waste liquid for 35 minutes, and obtain biochar tha...
Embodiment 2
[0037] A biochar-based helical magnetic biofilm reactor composed of such as figure 1 The spiral U-shaped groove track shown is composed of magnetic bio-carbon filler loaded in the spiral U-shaped groove track; the spiral U-shaped groove track is ascending, and the plane of the spiral U-shaped groove track is The angle with the horizontal plane is 15°, and the periphery of the spiral U-shaped groove track projected on the horizontal plane is a circle, and the diameter of the circle is 6 times the width of the spiral U-shaped groove track. The length to width ratio of the groove track is 30, and the depth is 12cm; the material of the spiral U-shaped groove track is stainless steel.
[0038] Wherein the preparation method of magnetic bio-carbon filler is:
[0039] (1) Add excessive waste iron scraps to the waste liquid containing sulfuric acid, add biochar after reacting for 30 minutes, stir for 15 minutes, absorb ferrous ions in the waste liquid for 40 minutes, and obtain bioch...
PUM
Property | Measurement | Unit |
---|---|---|
size | aaaaa | aaaaa |
porosity | aaaaa | aaaaa |
porosity | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com