Eureka AIR delivers breakthrough ideas for toughest innovation challenges, trusted by R&D personnel around the world.

Method for removing streak defects on hot rolled steel plate surface

A hot-rolled steel plate and mottled technology, used in workpiece surface treatment equipment, metal rolling, metal rolling, etc., can solve the problem of controlling the structure and thickness of the iron oxide scale on the surface of the steel plate. It does not involve how to eliminate the surface defects of the steel plate, etc. problems, to ensure the surface quality and mechanical properties, eliminate chromatic aberration defects, reduce the effect of difficulty

Active Publication Date: 2015-10-28
沈阳诚伟机械制造有限公司
View PDF6 Cites 6 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Chinese Patent Application No. 200710010183.5 "Medium and Thin Slab Continuous Casting and Rolling Strip Steel Surface Scale Control Method" provides the scale for medium and thin slab hot-rolled strip steel including composition design, descaling process, rolling and cooling process The control method is mainly aimed at the short-process production line of medium and thin slabs, and the main solution is how to remove the red rust on the surface. It does not mention how to eliminate the color difference defects after shot blasting on the surface of the steel plate
Chinese Patent Application No. 201010010116.5 "A Method for Detecting Scale Structure of Hot-Rolled Strip Steel by Chemical Corrosion" provides a chemical detection method for detecting the scale structure of hot-rolled strip steel, which is useful for controlling the structure and thickness of scale on the surface of steel plates wait did not introduce
Chinese Patent Application No. 201010189410.7 "Flexible Control Method of Scale on Hot-rolled Strip Surface" provides a method for controlling the structure and adhesion of scale on the surface of steel strip in a hot-rolled production line. Different processing characteristics are shown in the deep processing process. How to require different structure of iron oxide scale according to the deep processing process characteristics of downstream production enterprises (whether there is an oiling process) does not involve how to eliminate the surface defects of the steel plate

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Method for removing streak defects on hot rolled steel plate surface
  • Method for removing streak defects on hot rolled steel plate surface
  • Method for removing streak defects on hot rolled steel plate surface

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0027] (1) Heat the slab to 1200°C, then descale with high-pressure water, the descaling temperature is 1150°C, and the water pressure is 16MPa during descaling;

[0028] (2) rough rolling the descaled steel plate, the temperature of rough rolling is 1100℃;

[0029] (3) The rough-rolled steel plate is subjected to finish rolling, the finish rolling temperature is 950°C, and the roller table speed is 1.4m / s;

[0030] (4) After finishing rolling, laminar flow cooling is used for water cooling, and segmental cooling is adopted, the water ratio is 2.3; the cooling water volume is 150m3 / h; the temperature of the steel plate after cooling is 680°C;

[0031] (5) The water-cooled steel plate is cooled in the air on the cooling bed.

[0032] After the steel plate is rolled and water-cooled, the photo of cooling on the cooling bed is as follows figure 1 shown. from figure 1 It can be seen that after the steel plate is hot-rolled, there is no cracking phenomenon of iron oxide scale o...

Embodiment 2

[0034] (1) Heat the slab to 1220°C, then descale with high-pressure water, the descaling temperature is 1180°C, and the water pressure is at least 17MPa during descaling;

[0035] (2) rough rolling the descaled steel plate, the temperature of rough rolling is 1120°C;

[0036] (3) The rough-rolled steel plate is subjected to finish rolling, the finish rolling temperature is 960°C, and the roller table speed is 1.5m / s;

[0037] (4) After finishing rolling, laminar flow cooling is used for water cooling, and segmental cooling is adopted, the water ratio is 2.4; the cooling water volume is 200m3 / h; the temperature of reddening of the steel plate after cooling is 700°C;

[0038] (5) The water-cooled steel plate is cooled in the air on the cooling bed.

[0039] After the steel plate is rolled and water-cooled, the photo of cooling on the cooling bed is as follows image 3 shown. from image 3 It can be seen that when the steel plate is cooled on the cooling bed, the surface is s...

Embodiment 3

[0041] (1) Heat the slab to 1240°C, then descale with high-pressure water, the descaling temperature is 1200°C, and the water pressure is 19MPa during descaling;

[0042] (2) rough rolling the descaled steel plate, the temperature of rough rolling is 1180°C;

[0043] (3) The rough-rolled steel plate is subjected to finish rolling, the final rolling temperature of the finish rolling is 980°C, and the roller table speed is 1.7m / s;

[0044] (4) After finishing rolling, laminar flow cooling is used for water cooling, and segmental cooling is adopted, the water ratio is 2.5; the cooling water volume is 250m3 / h; the temperature of reddening of the steel plate after cooling is 730°C;

[0045] (5) The water-cooled steel plate is cooled in the air on the cooling bed.

[0046] After the steel plate is rolled and water-cooled, the photo of cooling on the cooling bed is as follows Figure 5shown. from Figure 5 It can be seen that under the process conditions of Example 3, the surface...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

PropertyMeasurementUnit
Thicknessaaaaaaaaaa
Login to View More

Abstract

The invention discloses a method for removing streak defects on a hot rolled steel plate surface and relates to a steel plate surface treatment method. The method comprises the following process: heating plate blank to 1200-1250 DEG C, and then, descaling by high pressure water at a descaling temperature of 1100-1200 DEG C, wherein water pressure required for descaling is at least 16 MPa; carrying out rough rolling on a descaled steel plate at a rough rolling temperature of 1100-1200 DEG C; carrying out finish rolling on the steel plate subjected to rough rolling, wherein a final rolling temperature of the finish rolling is 900-990 DEG C, and the speed of a roller way is 1.3-1.8m / s; after the finish rolling is ended, carrying out water-cooling by adopting a laminar cooling mode, and adopting sectional type cooling, wherein a water ratio is 2.2-2.6, the cooling water consumption is 150-250m<3> / h, and a red temperature of the cooled steel plate is 670-750 DEG C; and cooling the water-cooled steel plate in air at a cold bed. According to the method, oxide iron scale on the surface of the steel plate is easy to remove in a follow-up shot blasting process, thereby removing the streak defects on the steel plate surface subjected to shot blasting.

Description

technical field [0001] The invention relates to a steel plate surface treatment method, in particular to a method for eliminating mottled defects on the surface of a hot-rolled steel plate. Background technique [0002] The hot-rolled steel plate will produce a layer of oxide scale on the surface of the steel plate during the rolling process. Under different hot rolling conditions, the structure and thickness of the obtained iron oxide scale are changed. Hot-rolled sheets are playing an increasingly important role in the national economy, but the main concern is performance quality and dimensional accuracy. Surface quality has become a common problem in the industry that restricts the overall quality of hot-rolled sheets in my country. Due to the long-term lack of attention to the surface quality of hot-rolled steel products, these products often have problems such as red rust, pits and pits due to improper control of the surface iron sheet, causing many quality objections ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): B21B45/02B21B45/08B21B37/28
Inventor 孙彬曹光明刘振宇
Owner 沈阳诚伟机械制造有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Eureka Blog
Learn More
PatSnap group products