Method for preparing chrome tanning agent from waste chrome tanning liquid
A technology of chrome tanning agent and waste liquid, which is applied in the field of heavy metal recycling, can solve the problems of less applied research, and achieve the effects of reducing pollution, simple process operation, and high yield
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A method for preparing chrome tanning agent from the chrome tanning waste liquor of yellow cowhide soft surface leather comprises the following steps:
[0026] (1) After tanning, collect the waste chromium solution, adjust the pH of the waste chromium solution to 8 with sodium hydroxide to precipitate chromium, collect the chromium precipitate after standing, and then dehydrate the plate and frame filter to obtain chromium cake, and measure the chromium cake The water content is 65%, and the chromium trioxide is 12%.
[0027] (2) First weigh 100 parts of chromium cake, then weigh 25 parts of water, add 30 parts of 98% concentrated sulfuric acid to the solution, add the weighed chromium cake, heat up to 60°C, and stir for 30 minutes for hydrolysis. Then, cool down to room temperature and filter to remove impurities to obtain a filtrate, measure the concentration of 75g / L of chromium trioxide in the filtrate, and adjust the pH of the filtrate to 2.5. Use cation exchange ...
Embodiment 2
[0037] A kind of method of preparing chrome tanning agent from the chrome tanning waste liquid of producing sheepskin glove leather comprises the following steps:
[0038] (1) Collect the waste chrome solution after tanning, adjust the pH of the waste chrome solution to 9 with magnesia to precipitate the chromium, collect the chromium precipitate after standing, and then dehydrate the plate and frame filter to obtain the chromium cake, and measure the water content of the chromium cake Rate at 75%, chromium oxide 9%
[0039] (2) First weigh 100 parts of chromium cake, then weigh 20 parts of water, add 20 parts of 98% concentrated sulfuric acid to the solution, add the weighed chromium cake, slowly heat up to 65°C, and stir for 20 minutes for hydrolysis. Then, cool down to room temperature and filter to remove impurities to obtain a filtrate, measure the concentration of dioxide 65g / L of the filtrate, and adjust the pH of the filtrate to 2.0. Use cation exchange chromatography...
Embodiment 3
[0049] A kind of method for preparing chrome tanning agent from the chrome tanning waste liquid of producing pigskin garment leather comprises the following steps:
[0050] (1) After tanning, collect the waste chrome solution, adjust the pH of the waste chrome solution to 8.5 with sodium carbonate, make the chromium precipitate, collect the chromium precipitate after standing, and then dehydrate through the plate and frame filter press to obtain the chromium cake, and measure the water content of the chromium cake Rate 70%, Chromium Trioxide 10%
[0051] (2) Take 23 parts of water according to the weight percentage of chromium cake, add 26 parts of 98% concentrated sulfuric acid in the solution, add 100 parts of chromium cake, slowly heat up to 75 ° C, and stir for 15 minutes for hydrolysis reaction. Then, cool to room temperature and filter to remove impurities to obtain a filtrate, measure the chromium trioxide concentration 70g / L of the filtrate, and adjust the pH of the fi...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com