Repair and regeneration method for lithium cobaltate positive active material in waste lithium ion battery
A cathode active material, lithium-ion battery technology, applied in battery recycling, waste collector recycling, recycling technology and other directions, can solve the problems of secondary pollution of the atmospheric environment, high requirements for anticorrosion of leaching equipment, and many processing procedures. Achieve the effect of no secondary pollution, low equipment anti-corrosion requirements, and short process flow
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0026] Collect scrap lithium-ion batteries with lithium cobaltate as positive electrode material, place them in 1.0mol / L sodium hydroxide aqueous solution at room temperature for 2h discharge treatment; after discharge treatment, disassemble the scrap lithium-ion batteries to obtain Positive electrode sheet: according to the ratio (g / mL) of the mass of positive electrode sheet and the volume of ceramic crucible, positive electrode sheet is packed in the ratio of 1:15 in the ceramic crucible, is placed in box-type electric resistance furnace then and starts from room temperature with 5 ℃ / mL The heating rate of min raised the furnace temperature to 550°C and kept it warm for 20 minutes, then cut off the power of the box-type resistance furnace, and cooled it to room temperature naturally; took out the roasted positive electrode sheet, and according to the ratio of the mass of the positive electrode sheet to the volume of water (g / mL) is 1:50, put the positive electrode sheet int...
Embodiment 2
[0028] Collect scrap lithium-ion batteries with lithium cobaltate as positive electrode material, place them in 1.0mol / L sodium hydroxide aqueous solution at room temperature for 2h discharge treatment; after discharge treatment, disassemble the scrap lithium-ion batteries to obtain Positive electrode sheet: according to the ratio (g / mL) of the mass of positive electrode sheet and the volume of ceramic crucible, positive electrode sheet is packed in the ratio of 1:15 in the ceramic crucible, is placed in box-type electric resistance furnace then and starts from room temperature with 5 ℃ / mL The heating rate of min raised the furnace temperature to 550°C and kept it warm for 20 minutes, then cut off the power of the box-type resistance furnace, and cooled it to room temperature naturally; took out the roasted positive electrode sheet, and according to the ratio of the mass of the positive electrode sheet to the volume of water (g / mL) is 1:50, put the positive electrode sheet int...
Embodiment 3
[0030]Collect positive electrode scraps and positive electrode residues produced in the lithium-ion battery manufacturing process with lithium cobalt oxide as the positive electrode material to obtain the positive electrode sheet; Put the positive electrode piece into a ceramic crucible, and then place it in a box-type resistance furnace to raise the temperature of the furnace to 550 °C at a rate of 5 °C / min from room temperature and keep it for 20 min. Room temperature; take out the positive electrode sheet after roasting, put the positive electrode sheet into a container filled with water according to the ratio of the mass of the positive electrode sheet to the volume of water (g / mL) of 1:50 and stir with an electric stirrer at 50r / min Stir at a high speed for 20 minutes, and the temperature of the water during the stirring process is 30°C; after the stirring is stopped, sieve the mixture in the container with a 10-mesh sieve, the sieve is aluminum foil, and the sieve is a so...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com