Embodiment 1
[0056] The composition and weight ratio of the polymer hot-melt self-sealing sealing memory glue used in the process method of automobile wheel explosion-proof safety upgrade are as follows:
[0057] (1) Thermoplastic elastomer: 44%;
[0058] (2) Tackifier: 41%;
[0059] (3) Softener: 8%;
[0060] (4) Antioxidant: 1%;
[0061] (5) Filler: 5%;
[0062] (6) Cross-linking agent: 1%.
[0063] Among them, the thermoplastic elastomer is selected from SIS and SBS mixture; the tackifier is selected from terpene resin; the antioxidant is selected from the mixture of 264 and 300; the softener is selected from the mixture of naphthenic oil and dibutyl phthalate.
[0064] The process and steps of explosion-proof safety upgrade for automobile wheels are as follows:
[0065] First, use the air compression component (4), the inert medium production component (5), the raw material production component (6), and the auxiliary material production component (8) to respectively produce compre...
Embodiment 2
[0077] The composition and weight ratio of the polymer hot-melt self-sealing sealing memory glue used in the process method of automobile wheel explosion-proof safety upgrade are as follows:
[0078](1) Thermoplastic elastomer: 49%;
[0079] (2) Tackifier: 42%;
[0080] (3) Softener: 5%;
[0081] (4) Antioxidant: 1%;
[0082] (5) Filler: 2%;
[0083] (6) Cross-linking agent: 1%.
[0084] Among them, the thermoplastic elastomer is selected from SBS and SIS mixture; the tackifier is selected from terpene resin and terpene phenol resin; the antioxidant is selected from the mixture of 2246 and 300; the softener is selected from dibutyl phthalate and naphthenic oil mixture .
[0085] The process and steps of explosion-proof safety upgrade for automobile wheels are as follows:
[0086] First, use the air compression component (4), the inert medium production component (5), the raw material production component (6), and the auxiliary material production component (8) to respect...
Embodiment 3
[0098] The composition and weight ratio of the polymer hot-melt self-sealing sealing memory glue used in the process method of automobile wheel explosion-proof safety upgrade are as follows:
[0099] (1) Thermoplastic elastomer: 47%;
[0100] (2) Tackifier: 43.5%;
[0101] (3) Softener: 5%;
[0102] (4) Antiaging agent: 0.5%;
[0103] (5) Filler: 3%;
[0104] (6) Cross-linking agent: 1%.
[0105] Among them, the thermoplastic elastomer is selected from SIS; the tackifier is selected from terpene-styrene resin; the anti-aging agent is selected from the mixture of RD and 4010; the softener is selected from the mixture of aromatic oil and naphthenic oil.
[0106] The process and steps of explosion-proof safety upgrade for automobile wheels are as follows:
[0107] First, use the air compression component (4), the inert medium production component (5), the raw material rubber production component (6), and the auxiliary material production component (8) to make compressed air,...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com