Preparation method for filling materials in ultra-light warm clothes and application of filling material in ultra-light warm clothes
A technology for thermal clothing and fillers, applied in the application, clothing, clothing and other directions, can solve the problems of the conflict between thermal insulation and aesthetics, and achieve good application prospects, good compression performance, and good controllability.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment approach 1
[0025] Specific implementation mode one: the preparation method of the inner filler of the ultra-light thermal clothing in this embodiment is implemented according to the following steps:
[0026] 1. Preparation of graphene oxide: Add natural flake graphite into strong oxidizing mixed acid, stir for 10min-60min at a stirring speed of 100r / min-800r / min, then add strong oxidant permanganate in 3-10 times Potassium to prepare mixture A, then put mixture A in a water bath at 30°C to 80°C, and stir at a constant temperature for 4h to 20h at a stirring speed of 200r / min to 800r / min to obtain mixture B, and then mix mixture B Adding it into ice water, and adding hydrogen peroxide with a mass fraction of 30% to the ice water to obtain a graphite oxide suspension, washing with suction, centrifugal washing and drying, to obtain graphene oxide;
[0027] 2. Preparation of graphene oxide dispersion: Add the graphene oxide obtained in step 1 into deionized water and stir evenly to obtain a ...
specific Embodiment approach 2
[0036] Embodiment 2: The difference between this embodiment and Embodiment 1 is that the mass ratio of the volume of the strong oxidizing mixed acid described in step 1 to the natural flake graphite is (10mL-400mL): 1g. Other parameters are the same as in the first embodiment.
specific Embodiment approach 3
[0037] Specific embodiment three: the difference between this embodiment and specific embodiment one or two is that the strong oxidizing mixed acid described in step one consists of phosphoric acid with a mass fraction of 10% to 85% and sulfuric acid with a mass fraction of 10% to 98% by volume Ratio (3~10):1 composition. Other parameters are the same as those in Embodiment 1 or 2.
PUM
Property | Measurement | Unit |
---|---|---|
concentration | aaaaa | aaaaa |
quality score | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com