Application of benzoheterocycle alkaloids in preparation of marine organism stain preventing coatings
A marine biofouling and alkaloid technology, applied in antifouling/underwater coatings, biocide-containing paints, coatings, etc., can solve problems such as marine biofouling, impact, and hinder the exploration and utilization of marine resources , to achieve the effect of remarkable effect, remarkable anti-adhesion activity and good anti-marine biofouling activity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0017] Example 1: Anti-Marine Fouling Organism Brussel larvae Activity Test of Benzoalkaloid Compounds Represented by Formulas (1)-(5)
[0018] The activity test model adopts the adhesion inhibition test of Bugula neritina larvae, one of the most commonly used marine fouling biological models in the laboratory.
[0019] The collected mature B. multilocularis was placed in seawater filtered by a 0.22 μm filter membrane, stimulated by light, and the larvae produced by the mature B. multilocularis by light stimulation were collected. Larvae were placed in a watch glass containing seawater filtered through a 0.22 μm filter membrane. The activity test was done with the larvae produced by Bryosa larvae by light. Anti-larval settling activity of compounds was determined using 24-well polystyrene plates. The compound brevianamide F (Formula 1) was dissolved in DMSO and diluted with sterile filtered seawater to obtain solutions of different concentrations (1.65-50 μg / mL) as the test ...
Embodiment 2
[0022] Example 2: Field sea siding activity test of marine alkaloid compounds represented by combined formulas (1)-(5)
[0023]The field sea hanging board test adopts the traditional anti-fouling biological field sea hanging board test method. Dissolve 0.4g of the alkaloid compound mixture (molar ratio 1:1:1:1:1) containing formula (1)-(5) completely in 1mL of methanol, and then fully dissolve it with 10mL of resin containing 45%polyurethane After mixing, spread it on a dry PVC (10×10×0.3cm) board, hang it in the scallop culture area of Daya Bay, Shenzhen (114°32'59 east longitude, 22°40'37 north latitude) after air drying, and serve as the treatment group. Three parallels were set up for each treatment. Take 1ml of methanol and 10mL of resin containing 45%polyurethane and mix it and paint on the plate as a control. The hanging boards were taken out at the second and fourth month respectively, the types of fouling organisms were checked and the area percentage of the entir...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com