Composite biomass granular fuel and its processing technology
A biomass particle and processing technology, which can be applied to biofuels, waste fuels, fuels, etc., can solve the problems of high combustion slagging, unfavorable promotion and utilization, and low calorific value, so as to improve combustion quality, enhance environmental protection, The effect of calorific value increase
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] 20% peanut shells, 20% sawdust, 40% rice husks, 12% waste oil, 7% waste coal gangue powder, and 1% calcium oxide. First, crush peanut shells, wood chips and rice husks, and control the particle size between 1-2 mm, and then crush the coal gangue to within 0.5 mm; send the above-mentioned crushed raw materials into the mixing bin according to the ratio, and add oil and calcium oxide , mixed evenly, and sent to a granulator for compression; then sieved and packaged to obtain the product. The size of the obtained composite biomass particle fuel is generally cylindrical particles with a diameter of 6-10 mm and a length of 24-40 mm.
Embodiment 2
[0015] 15% of peanut shells, 15% of sawdust, 50% of rice husks, 9.5% of waste oil, 10% of waste coal gangue powder, and 0.5% of calcium oxide. First, crush peanut shells, wood chips and rice husks, and control the particle size between 1-2 mm, and then crush the coal gangue to within 0.5 mm; send the above-mentioned crushed raw materials into the mixing bin according to the ratio, and add oil and calcium oxide , mixed evenly, and sent to a granulator for compression; then sieved and packaged to obtain the product.
Embodiment 3
[0017] 18% peanut shells, 18.6% sawdust, 48.6% rice husks, 8% waste oil, 6% waste coal gangue powder, and 0.8% calcium oxide. First, crush peanut shells, wood chips and rice husks, and control the particle size between 1-2 mm, and then crush the coal gangue to within 0.5 mm; send the above-mentioned crushed raw materials into the mixing bin according to the ratio, and add oil and calcium oxide , mixed evenly, and sent to a granulator for compression; then sieved and packaged to obtain the product.
PUM
Property | Measurement | Unit |
---|---|---|
Diameter | aaaaa | aaaaa |
Length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com