Eureka AIR delivers breakthrough ideas for toughest innovation challenges, trusted by R&D personnel around the world.

Water-borne rust-based anticorrosion coating and preparation method thereof

A rust-proof, water-based technology, applied in anti-corrosion coatings, coatings, metal material coating processes, etc., can solve problems such as dead ends, high cost, and noise pollution in complex structural parts, and achieve good compatibility and stability , Long-term and efficient protection, the effect of prolonging the service life

Inactive Publication Date: 2013-07-03
ANHUI CHAOHU SOUTH MEMBRANE IND
View PDF5 Cites 10 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

At present, the anticorrosion of domestic steel structures still uses the old process of painting after sandblasting. Although the anticorrosion effect is good, there are also complex structural parts with dead angles in sandblasting and shot blasting processes, high power consumption, dust pollution, noise pollution, and cost. Therefore, it is very necessary to prepare rusty coatings that can be directly applied on rusty surfaces.
[0003] The traditional process uses phosphoric acid as a conversion agent. Although phosphoric acid can convert rust into a phosphating film, due to hydrogen precipitation, the paint film is prone to foaming, resulting in a decrease in adhesion

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0023] A kind of water-based anti-rust coating with rust, it is made up of the raw material of following parts by weight (kg):

[0024] Styrene-acrylic emulsion 70, water-based acrylic emulsion 40, alcohol ester dodeca film-forming aid 4, vanadium oxychloride 3, benzotriazole 0.8, glycerol 4, 2-methyl-1,3-propanediol 4, p- Hydroquinone 3, pyrocatechol 2, sodium ethylenediamine tetramethylene phosphonate 3, citric acid 4, modified binder 2, carboxymethyl cellulose 0.2, deionized water 55;

[0025] The preparation method of described modified binder is:

[0026] (1) Mix sodium metasilicate with 3-(methacryloyloxy)propyltrimethoxysilane by weight, 2% 1,2-bis(triethoxysilyl)ethane, 3% carboxy Sodium methylcellulose and 1% dicumyl peroxide are mixed and added to 15 times of the deionized water of the mixture, and stirred at a high speed of 1500 rpm to obtain a dispersion, which is dried and pulverized to obtain a powder;

[0027] (2) Ultrasonic disperse the powder obtained above ...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

PUM

No PUM Login to View More

Abstract

The invention discloses a water-borne rust-based anticorrosion coating which comprises the following raw materials by weight portion: 60-70 portions of styrene-acrylic emulsion, 30-40 portions of water-borne acrylic emulsion, 2-4 portions of alcohol ester-12 forming additive, 2-3 portions of vanadium oxytrichloride, 0.5-0.8 portions of benzotriazole, 3-4 portions of glycerine, 2-4 portions of 2- methyl-1,3- propylene glycol, 2-3 portions of hydroquinone, 1-2 portions of pyrocatechol, 2-3 portions of Ethylene Diamine Tetra Methylene Phosphonic Acid Sodium, 3-4 porptions of citric acid, 1-2 portions of modified adhesive, 0.1-0.2 portions of carboxymethyl cellulose and an appropriate amount of deionized water. The coating has good comprehensive performances including base body adhesive power, rot resistance, adhesive power, can completely avoid coating preprocessing processes, including sand blasting and shot-blasting, and can provide lasting and efficient protection for iron steels, the surfaces of which are rusty and not subjected to pre-processing; and accordingly, not only is the service life of an anti-corrosion finishing coat prolonged, but also the anti-corrosion coating process is simpler, and more efficient, economical and environment-friendly.

Description

technical field [0001] The invention mainly relates to a water-based paint, in particular to a water-based anti-rust paint with rust and a preparation method thereof. Background technique [0002] In order to protect steel from corrosion and prolong its service life, anti-corrosion coating on steel has become the most economical and effective method. In order to obtain excellent corrosion resistance, the rust on the steel must be removed before painting, otherwise the paint film and anti-corrosion effect will be poor due to the continuous expansion of the rust. Therefore, the rust removal treatment is an important part of the coating process Part, plays a decisive role in the success or failure of anti-corrosion coating. However, due to the limitation of construction conditions in the maintenance process of many large buildings, bridges, ships, and other complex steel structure components, it is difficult to use mechanized construction methods, and only manual or electr...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to View More

Application Information

Patent Timeline
no application Login to View More
IPC IPC(8): C09D125/14C09D133/00C09D7/12C09D5/08C23C22/50
Inventor 武道贵
Owner ANHUI CHAOHU SOUTH MEMBRANE IND
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Eureka Blog
Learn More
PatSnap group products