Detection method of damage of one-way silicon carbide fiber toughening silicon carbide ceramic matrix composite in oxidation environment
A silicon carbide fiber and composite material technology, applied in special data processing applications, instruments, electrical and digital data processing, etc. Overcome costly effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment Construction
[0026] The specific steps of the detection method for the damage of the unidirectional silicon carbide fiber toughened silicon carbide ceramic matrix composite material in the oxidizing environment of the present invention are as follows:
[0027] In the following, for a unidirectional SiC / SiC composite material subjected to an axial tensile stress of 800MPa in an air environment of 600°C and 100KPa, the material damage at different oxidation times is calculated. The radius R of the silicon carbide fiber bundle in the unidirectional SiC / SiC composite is 2 mm, and the thickness d of the carbon interface and the silicon carbide matrix is i 、d m 200μm and 800μm respectively, the width H of the matrix microcrack C The distance between adjacent microcracks, that is, the z-direction length L of the periodic microstructure is 16 mm. The performance parameters of each component material are shown in Table 1.
[0028] Table 1 Performance parameters of component materials
[0029] ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com