A technology of isophorone dicarbamate and isophorone diamine, which is applied in the field of preparation of isophorone dicarbamate, can solve the problems of expensive ionic liquids and increased production costs, and achieve The effect of easy separation and recycling, simple operation and mild reaction conditions
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] A kind of preparation method of isophorone dicarbamate, its concrete steps are:
[0026] (1) Add isophorone diamine dropwise to the mixed system of dimethyl carbonate and supported solid catalyst, react at 50°C for 16 hours, and filter; among them, dimethyl carbonate is 27g, isophorone diamine 17.0g, supported solid catalyst 0.88g.
[0027] (2) Add 3 times the volume of distilled water to the filtered filtrate, let it stand, filter, and dry to obtain 24.7 g of isophorone dicarbamate, with a yield of 86.3% and a purity of 97.1%.
[0028] The concrete preparation method of described supported type solid catalyst is:
[0029] (1) 33.1g Pb(NO 3 ) 2 Soluble in water, phosphoric acid adjusts the pH value to 3;
[0030] (2) Add 423.7g of carrier silica to the above aqueous solution, impregnate at room temperature for 2 hours, dry at 110°C for 6 hours, and bake at 580°C for 3 hours to obtain a supported solid catalyst PbO / SiO 2 , the active ingredient loading is 5wt%.
Embodiment 2
[0032] A kind of preparation method of isophorone dicarbamate, its concrete steps are:
[0033] (1) Add isophorone diamine dropwise to the mixed system of dimethyl carbonate and supported solid catalyst, react at 55°C for 12 hours, and filter; among them, dimethyl carbonate is 90g, isophorone diamine 17.0g, supported solid catalyst 10.7g.
[0034] (2) Add 10 times the volume of distilled water to the filtered filtrate, let it stand, filter, and dry to obtain 25.3 g of isophorone dicarbamate, with a yield of 88.5% and a purity of 98.2%.
[0035] The concrete preparation method of described supported type solid catalyst is:
[0036] (1) 33.1g Pb(NO 3 ) 2 Soluble in water, phosphoric acid adjusts the pH value to 3.1;
[0037] (2) Add 52g of carrier alumina to the above aqueous solution, impregnate at room temperature for 2.5 hours, dry at 100°C for 4 hours, and roast at 450°C for 5 hours to obtain a supported solid catalyst PbO / Al 2 o 3 , The active component loading is 30w...
Embodiment 3
[0039] A kind of preparation method of isophorone dicarbamate, its concrete steps are:
[0040] (1) Add isophorone diamine dropwise to the mixed system of dimethyl carbonate and supported solid catalyst, react at 60°C for 9 hours, and filter; among them, dimethyl carbonate is 54 g, isophorone diamine 17.0 g of amine, 4.26 g of supported solid catalyst.
[0041] (2) Add 6 times the volume of distilled water to the filtered filtrate, let it stand, filter, and dry to obtain 25.0 g of isophorone dicarbamate, with a yield of 87.3% and a purity of 96.8%.
[0042] The concrete preparation method of described supported type solid catalyst is:
[0043] (1) 29.7g Zn (NO 3 ) 2 ·6H 2 O is dissolved in water, and phosphoric acid adjusts the pH value to 3.2;
[0044] (2) Add 32.56g of carrier silica to the above aqueous solution, soak at room temperature for 3 hours, dry at 110°C for 8 hours, and bake at 480°C for 4 hours to obtain a supported solid catalyst ZnO / SiO 2 , The active com...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com