Embodiment 1
[0023] Preparation steps of heating fiber:
[0024] 40%wt eks fiber and 60%wt acrylic fiber are blended into heating fiber, the yarn count of heating fiber is 40 twists, that is, the yarn density of heating fiber is 14.8tex, that is, the yarn weight of heating fiber per 1000 meters is 14.8g . The eks fiber used in this example is produced by Japan Sanrayon Co., Ltd.
[0025] Hygroscopic fiber preparation steps:
[0026] 30%wt acrylic fiber and 70wt% viscose fiber are blended into hygroscopic fiber, the yarn count of hygroscopic fiber is 40 twists, that is, the yarn density of hygroscopic fiber is 14.8tex, that is, the yarn weight of every 1000 meters of hygroscopic fiber is 14.8g .
[0027] Weaving steps:
[0028] Using the threading method of 1 thread and 6 holes, weave the heating fiber into the inner layer fabric; and make the mesh density of the inner layer fabric 12 meshes / cm.
[0029] Adopt the threading method of 1 thread and 6 holes to weave the moisture-absorbing...
Embodiment 2
[0041] Preparation steps of heating fibers: same as in Example 1.
[0042] Hygroscopic fiber preparation steps:
[0043] The blending of 40%wt acrylic fiber and 60wt% viscose into hygroscopic fiber, the yarn count of hygroscopic fiber is 40 twists, that is, the yarn density of hygroscopic fiber is 14.8tex, that is, the yarn weight of every 1000 meters of hygroscopic fiber is 14.8g .
[0044] Weaving steps:
[0045] Using the threading method of 1 thread and 6 holes, weave the heating fiber into the inner layer fabric; and make the mesh density of the inner layer fabric 16 meshes / cm.
[0046] Using the threading method of 1 thread and 6 holes, weave the moisture-absorbing fiber into the outer layer fabric; and make the mesh density of the outer layer fabric 16 meshes / cm.
[0047] The inner layer fabric and the outer layer fabric are sewn together by a tuck process, and an air layer is formed between the inner layer fabric and the outer layer fabric, thereby obtaining a heat-...
Embodiment 3
[0050] Preparation steps of heating fibers: same as in Example 1.
[0051] Hygroscopic fiber preparation steps:
[0052]The blending of 50%wt acrylic fiber and 50wt% viscose into hygroscopic fiber, the yarn count of hygroscopic fiber is 40 twists, that is, the yarn density of hygroscopic fiber is 14.8tex, that is, the yarn weight of every 1000 meters of hygroscopic fiber is 14.8g .
[0053] Weaving steps:
[0054] Using the threading method of 1 thread and 6 holes, weave the heating fiber into the inner layer fabric; and make the mesh density of the inner layer fabric 14 meshes / cm.
[0055] Adopt the threading method of 1 thread and 6 holes to weave the moisture-absorbing fiber into the outer layer fabric; and make the mesh density of the outer layer fabric 14 meshes / cm.
[0056] The inner layer fabric and the outer layer fabric are sewn together by a tuck process, and an air layer is formed between the inner layer fabric and the outer layer fabric, thereby obtaining a heat...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com