Embodiment 1
[0035] A rope with a white body and a purple-red end, which consists of a white body and a purple-red ink-impregnated end. (see figure 1 )
[0036] The preparation method is as follows:
[0037] 1. Blending of sizing paste, ink and gloss paste:
[0038] 1.1 Preparation of sizing paste: 40 parts of polyurethane resin, 10 parts of trimethylbenzene, 50 parts of aliphatic amine catalyst, 30 parts of dimethyl succinate solvent, and 1 part of defoamer. After 0.5h complete defoaming, it is ready for use;
[0039] 1.2 Preparation of ink: 80 parts of polyurethane resin, 20 parts of trimethylbenzene, 7 parts of organic pigment, 25 parts of dimethyl succinate solvent, and 1.5 parts of defoamer. After mixing, let it stand for about 16 hours to completely defoam reserve;
[0040] 1.3 Preparation of gloss paste: 45 parts of polyurethane resin, 10 parts of trimethylbenzene, 8 parts of corresponding aliphatic amine catalysts, 50 parts of dimethyl succinate solvent, and 1.5 parts of defoa...
Embodiment 2
[0047] A rope with a black body and black ends, comprising a black body and a black ink-impregnated end. (see figure 2 )
[0048] The preparation method is as follows:
[0049] 1. Blending of sizing paste, ink and gloss paste:
[0050]1.1 Preparation of setting paste: 45 parts of polyurethane resin, 5 parts of trimethylbenzene, 40 parts of aliphatic amine catalyst, 25 parts of dimethyl succinate solvent, and 2 parts of defoamer. Use after 1h complete defoaming;
[0051] 1.2 Ink formula: 90 parts of polyurethane resin, 10 parts of trimethylbenzene, 8 parts of organic pigment, 20 parts of dimethyl succinate solvent, and 1 part of defoamer. After mixing and stirring, let it stand for about 20 hours to completely defoam use;
[0052] 1.3 Glossy surface paste formula: 40 parts of polyurethane resin, 5 parts of trimethylbenzene, 5 parts of aliphatic amine catalyst, 40 parts of dimethyl succinate solvent, 2 parts of defoamer. Use after 0.6h complete defoaming;
[0053] 2. Rop...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com